| Literature DB >> 30205600 |
Zahra Bazrafshan1, George K Stylios2.
Abstract
A collagen-based copolymer,Entities:
Keywords: biocomposite; casting; collagen; electrospinning; graphene; mechanical testing; physical properties
Year: 2018 PMID: 30205600 PMCID: PMC6163636 DOI: 10.3390/nano8090703
Source DB: PubMed Journal: Nanomaterials (Basel) ISSN: 2079-4991 Impact factor: 5.076
The effect of graphene oxide (GO) contents on grafting parameters.
| Sample | Comonomer Cont. in Feed | EA Cont. | Initiator | GO (13 mg mL−1) | Nitrogen Content (%) | ||
|---|---|---|---|---|---|---|---|
| S1 | 54.91 | 0.5 | 4.51 | 0 | 16.09 | 30.67 | 7.46 |
| 8.00 | 68.7 | 97.63 | 6.32 | ||||
| 16.00 | 94.47 | 97.42 | 6.03 | ||||
| S2 | 109.85 | 5.00 | 9.10 | 0 | 46.48 | 36.74 | 6.86 |
| 8.00 | 101.66 | 94.02 | 5.65 | ||||
| 16.00 | 108.93 | 87.90 | 5.96 |
Figure 1TEM image of few-layer Graphene oxide that (Black arrows) stacked on top of one another. The scale bar shown on the bottom bar is 500 nm.
Figure 2Fourier Transform Infrared Spectroscopy (FT-IR) Transmittance vs. frequency for ASC-g-P(MMA-co-EA) with/without graphene oxide (GO) contents; to clarify, curves associated with comonomer feed ratios were demonstrated, as following: (a) composite films of lower comonomer feed ratio and (b) composite films of higher comonomer feed ratio.
Figure 3UV-Vis spectra of composite films from GO-ASC-g-P(MMA-co-EA) suggesting π–π stacking of the components with increasing GO contents.
Figure 4Heat flow vs. temperature of composite films from ASC-g-P(MMA-co-EA) with/without GO contents, in Differential Scanning Calorimeter (DSC) heating phase with the rate of 10 °C min−1 in an aluminum pan. To clarify, curves associated with the decomposition transition of GO contents were demonstrated in the same graph happening within the temperature ranges between 190–280 °C) in samples with high GO contents.
Figure 5Thermogravimetric analysis (TGA) graph of weight change as a function of temperature for composite films from ASC-g-P(MMA-co-EA) with GO contents.
Figure 6(1) Investigation of cross-sectional morphology of porous composite films of ASC-g-P(MMA-co-EA) without GO contents: (a) F1-0, (b) F2-0; the multilayer nanostructure of ASC-g-P(MMA-co-EA) with GO contents: (c) F1-8, (d) F1-16, (e) F2-8, (f) F2-16; and, (2) the color appearances of nanocomposite films on a light blue substrate.
Mechanical properties of samples.
| Samples | Tensile Stress (N/mm2) | Tensile Strain (mm/mm) | Tenacity (N/mm2) | Breaking Stress (N/mm2) | Breaking Strain (mm/mm) | Modules (CN/mm2) |
|---|---|---|---|---|---|---|
| F1-8 | 6.42 ± 0.96 | 0.20 ± 0.15 | 15.11 ± 2.57 | 6.00 ± 0.90 | 0.31 ± 0.05 | 84.52 ± 13.13 |
| F1-16 | 1.02 ± 0.20 | 0.19 ± 0.04 | 2.72 ± 0.54 | 0.86 ± 0.17 | 0.26 ± 0.06 | 14.66 ± 2.93 |
| F2-8 | 7.00 ± 1.40 | 0.17 ± 0.09 | 16.66 ± 1.87 | 6.99 ± 0.70 | 0.17 ± 0.16 | 107.85 ± 9.79 |
| F2-16 | 4.11 ± 0.49 | 0.17 ± 0.02 | 9.95 ± 1.31 | 3.66 ± 0.44 | 0.19 ± 0.04 | 61.41 ± 7.73 |
| F1-0 | 0.99 ± 0.09 | 0.18 ± 0.08 | 2.63 ± 0.24 | 0.71 ± 0.06 | 0.19 ± 0.02 | 14.31 ± 1.29 |
| F2-0 | 1.23 ± 0.07 | 0.25 ± 0.05 | 3.28 ± 0.20 | 1.13 ± 0.07 | 0.26 ± 0.03 | 13.37 ± 0.80 |
Figure 7A representative stress-strain curve recorded from tensile test of composite films from ASC-g-P(MMA-co-EA) with/without GO contents.
Figure 8(a) The water contact angle vs. time after 10 s and 10 min; (b) water absorption (hydration degree) and mass loss after incubation time of 12 h at room temperature; (c) Water absorption capacity of the samples as a function of temperature in percentage; and, (d) Mass residual percentage vs. incubation time (week).
Figure 9The effect of the GO contents on the mean fiber diameter and the uniformity (standard deviation value) of the electrospun fiber from the GO-ASC -g-P(MMA-co-EA nanocomposite: SEM images of (a) M1-8; (b)M1-16; (c) M2-8; and, (d) M2-16; the scale bar shown on the bottom bar is 10 µm.
Figure 10The arrangement of GO in the electrospun fiber from the GO-ASC-g-P(MMA-co-EA nanocomposite: TEM images of (a) M1-8, (b) M1-16, (c) M2-8; and, (d) M2-16. The scale bar shown on the bottom bar is 500 nm.