| Literature DB >> 29267524 |
Manuela Gonçalves de Souza E Silva1, Eliseu Aldrighi Münchow1, Rafael Pino Vitti2,3, Mário Alexandre Coelho Sinhoreti3, Evandro Piva1, Fabrício Aulo Ogliari4, Cesar Henrique Zanchi1.
Abstract
The aim of this study was to synthesize and evaluate physicochemical properties of a new salicylate derivative in experimental calcium-based root canal sealers. Two salicylate derivatives were synthesized for the transesterification reaction of methyl salicylate with two different alcohols (1,3-butylenoglicol disalicylate-BD and pentaerythritol tetrasalicylate -PT) in molar ratio 1:3 and 1:6, respectively. The products (BD and PT), were characterized by Fourier Transform Infrared Spectroscopy (FTIR) and Nuclear Magnetic Resonance spectroscopy (RMN). Calcium-based experimental sealers were prepared with the same catalyst paste (60% of MTA, 39% of n-ethyl-o-toluenesulfonamide, and 1% titanium dioxide) and four different concentrations of BD and PT in the base pastes (40/0 - control, 35/5, 30/10 and 20/20) with 60% of bismuth oxide. The experimental sealers were evaluated for setting time, solubility (24 h, 7, 14 and 30 days), diametral tensile strength and Young's Modulus. Data were analyzed by one- or two-way ANOVA with Tukey's test (p<0.05). The addition of PT reduced the materials setting time. After 24 h the sealer 40/0 and 35/5 had higher solubility, and after 14 and 28 days the sealer 20/20 showed the lowest solubility (p<0.05). After 7 days the sealer 20/20 stabilized its solubility. The sealer 40/0 presented the highest values and the 20/20 presented the lowest values of diametral tensile strength and Young's modulus (p<0.05). The addition of PT to calcium-based root canal sealers provides benefits to the setting time and solubility.Entities:
Mesh:
Substances:
Year: 2018 PMID: 29267524 DOI: 10.1590/0103-6440201801441
Source DB: PubMed Journal: Braz Dent J ISSN: 0103-6440