| Literature DB >> 29016985 |
Dimitrios Mavreas1, Jean-François Cuzin1, Guillaume Boonen1, Bart Vande Vannet1.
Abstract
Objectives: The aim of this paper was to compare failure differences in precious metal customized lingual brackets bonded with three adhesive systems. Also, differences in failure of non-precious metal brackets with and without a silicatized base layer bonded with the same adhesive, as well as the influence of enamel etching prior to using a self-etching dual cure resin were explored. Materials/methods: Five different groups were defined in a semi-randomized approach. Group 1 (IME): Maxcem Elite with 378 Incognito brackets and etched teeth, Group 2 (IMNE): Maxcem Elite with 193 Incognito brackets on non-etched teeth, Group 3 (INE): Nexus+Excite with 385 Incognito brackets, Group 4 (IRE): Relyx with 162 Incognito brackets, Group 5 (HRME) and Group 6 (HNRME): Maxcem Elite with 182 Harmony brackets with silicatized and non-slicatized bases respectively. Bracket failures were recorded over a 12-month period.Entities:
Mesh:
Substances:
Year: 2018 PMID: 29016985 DOI: 10.1093/ejo/cjx055
Source DB: PubMed Journal: Eur J Orthod ISSN: 0141-5387 Impact factor: 3.075