Color stability of lithium disilicate ceramics after aging and immersion in common beverages.

Eleni-Sotiria Palla1, Eleana Kontonasaki2, Nikolaos Kantiranis3, Lambrini Papadopoulou4, Triantafyllia Zorba5, Konstantinos M Paraskevopoulos6, Petros Koidis7.   

Abstract

STATEMENT OF PROBLEM: The color of an esthetic restoration and its color stability are important for long-term success. However, the impact of common beverages on lithium disilicate ceramic is not well known.
PURPOSE: The purpose of this in vitro study was to investigate color variations of lithium disilicate ceramics after thermocycling (TC) and immersion in commonly consumed beverages.
MATERIAL AND METHODS: A total of 288 specimens (1×10×10 mm) were fabricated from IPS e-max computer-aided design (CAD) (n=72), IPS e-max CERAM ([CER] n=72), IPS e-max Press with glazing ([PG] n=72), and IPS e-max Press without glazing ([PNG] n=72) according to the manufacturer's instructions. Each group was divided into 4 subgroups (n=18): TC, coffee, black tea, and red wine. Thermocycling was performed at 21 900 cycles at 5°C, 37°C, 55°C, and 37°C (3 years' clinical simulation), whereas the specimens were soaked in the staining solutions for up to 54 hours (3 years' clinical simulation). Color parameters L*, a*, and b* were assessed with an ultraviolet-visible spectroscopy recording spectrophotometer. Color difference (ΔE) was calculated using the equation [ΔΕ= [(ΔL*)2 + (Δa*)2 + (Δb*)2]½]. Intraexaminer reliability was assessed by using the intraclass correlation coefficient. Two-way analysis of variance was used for the analysis of ΔΕ, and the parameters L*, a*, and b* were analyzed with linear mixed models for repeated measurements and the Bonferroni pair-wise comparison test (α=.05).
RESULTS: Parameters ΔΕ, L*, a*, and b* were significantly affected by the interaction between material and treatment (P<.001). A ΔΕ >1 was recorded for PG with tea, wine, and coffee, PG after TC and CER after TC. For L*, greater reduction was observed for PNG with tea and CER after TC, whereas for a* significant changes were positive (to red shades), except for PNG with TC, where PNG with wine showed the greatest positive change. For b*, significant changes were negative (to blue shades) except for PNG with tea and coffee and CAD with tea.
CONCLUSIONS: All groups demonstrated color changes below the clinically perceptible level (ΔΕ<3.7), except PNG in tea which showed statistically significant color differences (ΔΕ>4). CAD presented higher color stability compared with the nonglazed Press specimens.
Copyright © 2017 Editorial Council for the Journal of Prosthetic Dentistry. Published by Elsevier Inc. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2017        PMID: 28923549     DOI: 10.1016/j.prosdent.2017.04.031

Source DB:  PubMed          Journal:  J Prosthet Dent        ISSN: 0022-3913            Impact factor:   3.426


  9 in total

1.  Effect of surface finishing treatments on the color stability of CAD/CAM materials.

Authors:  Funda Ozen; Nermin Demirkol; Ozge Parlar Oz
Journal:  J Adv Prosthodont       Date:  2020-06-18       Impact factor: 1.904

2.  Impact of thermocycling on surface roughness, microhardness and optical properties of three different lithium disilicate ceramics.

Authors:  Ahmad M Al-Thobity; Abdulkareem M AlOtaibi; Abdulrahman E Alhumaidan; Ahmed A Aldossary; Intisar Ahmad Siddiqui; Mohamed Ahmed Helal; Abdulmohsen Alsalman
Journal:  Saudi Dent J       Date:  2022-08-11

3.  Influence of electronic nicotine delivery systems (ENDS) in comparison to conventional cigarette on color stability of dental restorative materials.

Authors:  Fahim Vohra; Abdulelah F Andejani; Osamah Alamri; Abdulaziz Alshehri; Rana S Al-Hamdan; Thamer Almohareb; Tariq Abduljabbar
Journal:  Pak J Med Sci       Date:  2020 Jul-Aug       Impact factor: 1.088

4.  The Effect of Aging on Composition and Surface of Translucent Zirconia Ceramic.

Authors:  Korina Mešić; Igor Majnarić; Jasmina Obhođaš; Gorana Baršić; Ketij Mehulić
Journal:  Acta Stomatol Croat       Date:  2020-12

5.  The Effect of Smoking and Brushing on the Color Stability and Stainability of Different CAD/CAM Restorative Materials.

Authors:  Stuart Schelkopf; Caroline Dini; Thamara Beline; Alvin G Wee; Valentim A R Barão; Cortino Sukotjo; Judy Chia-Chun Yuan
Journal:  Materials (Basel)       Date:  2022-10-05       Impact factor: 3.748

6.  The effect of prolonged holding time on the mechanical property and microstructural property of lithium disilicate glass-ceramic.

Authors:  Feng Lin; Bin Wang; Yanmei Zhang; Shuigen Li; Qiufang Zhang; Yin Xiao; Qiliang Zuo
Journal:  J Mater Sci Mater Med       Date:  2022-10-03       Impact factor: 4.727

7.  Effect of Aging on the Microstructure and Optical Properties of Translucent ZrO 2 Ceramics.

Authors:  Korina Mešić; Igor Majnarić; Ketij Mehulić
Journal:  Acta Stomatol Croat       Date:  2021-06

8.  Effects of Khat on Surface Roughness and Color of Feldspathic and Zirconia Porcelain Materials under Simulated Oral Cavity Conditions.

Authors:  Mohammed M Al Moaleem; Rashad AlSanosy; Nasser M Al Ahmari; Mansoor Shariff; Abdulkhaliq A Alshadidi; Hassan A Alhazmi; Asaad Khalid
Journal:  Medicina (Kaunas)       Date:  2020-05-13       Impact factor: 2.430

9.  Effect of Hydrothermal Aging and Beverages on Color Stability of Lithium Disilicate and Zirconia Based Ceramics.

Authors:  Satheesh B Haralur; Noura Raqe S Alqahtani; Fatimah Alhassan Mujayri
Journal:  Medicina (Kaunas)       Date:  2019-11-19       Impact factor: 2.430

  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.