Fan Fan1,2, Muhammad Ibrahim1,2, Panpan Dai1,2, Yixin Mao1,2, Bing He3, Gang Wu4, Jianfeng Ma1,2, Shengbin Huang1,2,4.
Abstract
The aim of this study was to evaluate the effect of maleic acid (MA) on both the bond strength of fibre post to root dentine and smear layer removal after post space preparation. Sixty, single-canal premolars were endodontically treated and randomly assigned to four groups: group 1 [0.9% saline solution (control]); group 2 [2.5% sodium hypochlorite (NaOCl)]; group 3 [17% ethylenediaminetetraacetic acid (EDTA) followed by 2.5% NaOCl]; and group 4 (7% MA followed by 2.5% NaOCl). Self-adhesive resin cement was used to test the adhesion of a glass-fibre post to the root dentine through a micropush-out test. Scanning electron microscopy was performed to examine and score the treated specimens for smear layer removal, and stereomicroscopy was applied to investigate the failure modes of fibre posts. Maleic acid exhibited the highest mean bond-strength values in the apical regions among all the groups. Most failure modes (31.9%) were adhesive-type failures between the dentine and luting materials. Maleic acid performed statistically significantly better than the other groups regarding smear layer removal, especially in the apical region. Maleic acid is an effective irrigant that can remove the smear layer, open dentinal tubules, and act as a high-efficiency final irrigant in activation protocols.Entities:
Keywords: irrigation; post space preparation; push-out; resin cement; smear layer
Mesh:
Substances:
Year: 2017 PMID: 28782855 DOI: 10.1111/eos.12365
Source DB: PubMed Journal: Eur J Oral Sci ISSN: 0909-8836 Impact factor: 2.612