| Literature DB >> 28621710 |
Pedro Leo1, Gisela Orcajo2, David Briones3, Guillermo Calleja4, Manuel Sánchez-Sánchez5, Fernando Martínez6.
Abstract
The activity and recyclability of Cu-MOF-74 as a catalyst was studied for the ligand-free C-O cross-coupling reaction ofEntities:
Keywords: 4-formyldiphenyl ether; 4-nitrobenzaldehyde; MOF; O-arylation reaction; catalyst; ligand-free; phenol; recyclable Cu-MOF-74
Year: 2017 PMID: 28621710 PMCID: PMC5485796 DOI: 10.3390/nano7060149
Source DB: PubMed Journal: Nanomaterials (Basel) ISSN: 2079-4991 Impact factor: 5.076
Figure 1Catalyst characterization of Cu-MOF-74: (a) PXRD patterns; (b) SEM images; (c) nitrogen adsorption–desorption isotherms at −196 °C with an inset showing the micropore size distribution curve as generated by NL-DFT method, and (d) TGA under inert atmosphere.
Figure 2Kinetics of 4-nitrobenzaldehyde (NB) conversion catalyzed by Cu-MOF-74 at different temperatures
Figure 3NB conversion in the absence of catalyst (blank), in the presence of Cu-MOF-74 catalyst for 120 min and in the presence of Cu-MOF-74 for 5 min and subsequent removal.
Figure 4NB conversion vs. reaction time given by Cu-MOF-74 catalyst at different NB/Ph ratios.
Figure 5NB conversion vs. reaction time given by different concentration of Cu-MOF-74.
Figure 6NB conversion vs. reaction time given by Cu-MOF-74 catalysts in different solvents.
Figure 7NB conversion vs. reaction time given by Cu-MOF-74 catalysts in the absence of base and in the presence of different bases.
Figure 8NB conversion vs. reaction time given by Cu-MOF-74 catalysts at different K2CO3 concentrations.
Figure 9NB conversion vs. reaction time using different substituted-phenols.
Figure 10NB conversion vs. reaction time using different nitroarenes.
Figure 11NB conversion vs. reaction time given by different homogeneous and heterogeneous Cu-based catalysts.
Figure 12(a) PXRD patterns; (b) nitrogen adsorption–desorption isotherms at −196 °C of nano sized- and micron sized-Cu-MOF-74.
Textural properties of nano- and micro-Cu-MOF-74 materials.
| Cu-MOF-74 | Crystal Size (nm) | SBET (m2/g) | SExternal c (m2/g) |
|---|---|---|---|
| Nanocrystalline | 14 a | 1103 | 286 |
| Microcrystalline | 10,000 b | 1126 | 124 |
a Estimated by Scherrer equation. b Estimated by SEM. c Estimated by t-plot method.
Figure 13NB conversion vs. reaction time given by nano- and micron-sized Cu-based catalysts.
Figure 14Catalytic activity of Cu-MOF-74 catalyst after several reaction cycles.
Figure 15XRD patterns of Cu-MOF-74 catalyst after several reaction cycles.
Scheme 1C–O cross-coupling reaction of phenol with 4-nitrobenzaldehyde.