Marginal Adaptation, Gap Width, and Fracture Strength of Teeth Restored With Different All-Ceramic Vs Metal Ceramic Crown Systems: An in Vitro Study.

Carlo Monaco1, Martin Rosentritt2, Altin Llukacej1, Paolo Baldissara1, Roberto Scotti1.   

Abstract

This study evaluated marginal adaptation before and after thermomechanical (TCML) loading, gap width and fracture strength of all-ceramic single crowns, as compared to porcelain-fused-to-metal (PFM). Thirty extracted premolars were prepared with a round shoulder of 1.0 mm depth. Specimens were restored with zirconia-ceramic (Group 1), lithium disilicate (Group 2) and metal-ceramic single crowns (Group 3). The replica of each sample was observed with a scanning electron microscope (SEM) to evaluate the crown-cement (c-c) and tooth-cement interface (t-c). After TCML, perfect margins decreased to 91.3% (c-c) and 93.9% (t-c) in Group 1, 94.6% (c-c) and 96.0% (t-c) in Group 2 and 73.5% (c-c) and 53.1% (t-c) in Group 3. The mean fracture strengths were 654.8 ± 98.1 N for Group 1, 551.3 ± 127 N for Group 2 and 501.43 ± 110.1 N for Group 3. All-ceramic systems could substitute for metal-ceramic crowns, but chipping of veneering ceramics, especially in zirconia-based crowns, should be investigated. Copyright
© 2016 Dennis Barber Ltd.

Entities:  

Keywords:  All-Ceramic System; CAD/CAM System; Fracture Strength; Lithium Disilicate; Marginal Adaptation; Private-Label; Zirconiazzm321990

Mesh:

Substances:

Year:  2016        PMID: 28509504     DOI: 10.1922/EJPRD_01550Monaco08

Source DB:  PubMed          Journal:  Eur J Prosthodont Restor Dent        ISSN: 0965-7452


  5 in total

1.  IPS e.max for All-Ceramic Restorations: Clinical Survival and Success Rates of Full-Coverage Crowns and Fixed Partial Dentures.

Authors:  Silvia Brandt; Anna Winter; Hans-Christoph Lauer; Fritz Kollmar; Soo-Jeong Portscher-Kim; Georgios E Romanos
Journal:  Materials (Basel)       Date:  2019-02-02       Impact factor: 3.623

Review 2.  Current status on lithium disilicate and zirconia: a narrative review.

Authors:  Fernando Zarone; Maria Irene Di Mauro; Pietro Ausiello; Gennaro Ruggiero; Roberto Sorrentino
Journal:  BMC Oral Health       Date:  2019-07-04       Impact factor: 2.757

3.  The Effect of Finish Line Design on the Fracture Strength of Zirconia Copings.

Authors:  Zahra Hashemi Ardakani; Sahar Khorsandipour; Mina Mohaghegh; Seyed Ahmad Ghoreishian; Amir Ali Reza Khaledi
Journal:  J Dent (Shiraz)       Date:  2019-12

4.  Color matching of full ceramic versus metal-ceramic crowns - a spectrophotometric study.

Authors:  Delia Cristina Greţa; Cristina Gasparik; Horaţiu Alexandru Colosi; Diana Dudea
Journal:  Med Pharm Rep       Date:  2020-01-31

Review 5.  Comparative Assessment of the Functional Parameters for Metal-Ceramic and All-Ceramic Teeth Restorations in Prosthetic Dentistry-A Literature Review.

Authors:  Ana Ispas; Laura Iosif; Daniela Popa; Marius Negucioiu; Mariana Constantiniuc; Cecilia Bacali; Smaranda Buduru
Journal:  Biology (Basel)       Date:  2022-04-05
  5 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.