Literature DB >> 28054502

Enhanced pH stability, cell viability and reduced degradation rate of poly(L-lactide)-based composite in vitro: effect of modified magnesium oxide nanoparticles.

Jinjun Yang1,2, Xiuxiang Cao1, Yun Zhao1,3, Liang Wang3, Bei Liu1, Junping Jia1, Hui Liang1, Minfang Chen1,3.   

Abstract

The modified MgO nanoparticles (m-MgO-NPs) by a copolymer containing the malic acid and low molecular weight poly(L-lactide) (poly(L-lactide-co-malic acid), PLMA) have been successfully prepared. MgO nanoparticles (MgO-NPs) were coated by the PLMA and m-MgO-NPs were uniformly dispersed in the PLLA matrix to a novel biocomposite material (PLLA/m-MgO-NPs) with more excellent interface bonding and uniformer dispersion, compared to the PLLA/MgO-NPs. Compared to neat PLLA and PLLA/MgO-NPs film, the m-MgO-NPs not only shown the obvious neutralization effect on the acidic solution in the degradation of the PLLA and better hydrophilicity, but also exhibited the higher cell viability and decrease the toxicity to the cell in the degradation process of PLLA in vitro. In addition, m-MgO-NPs also reduced the degradation rate of the PLLA. The mechanisms for the excellent dispersion of nanoparticles, enhanced pH stability, reduced degradation rate of the PLLA and the cell viability in vitro in the case of PLLA/m-MgO-NPs have also been proposed and discussed in detail.

Entities:  

Keywords:  Poly(L-lactide); in vitro; magnesium oxide nanoparticle; modification

Mesh:

Substances:

Year:  2017        PMID: 28054502     DOI: 10.1080/09205063.2017.1279534

Source DB:  PubMed          Journal:  J Biomater Sci Polym Ed        ISSN: 0920-5063            Impact factor:   3.517


  3 in total

1.  Biomimetic mineralized strontium-doped hydroxyapatite on porous poly(l-lactic acid) scaffolds for bone defect repair.

Authors:  Min Ge; Kun Ge; Fei Gao; Weixiao Yan; Huifang Liu; Li Xue; Yi Jin; Haiyun Ma; Jinchao Zhang
Journal:  Int J Nanomedicine       Date:  2018-03-20

2.  The Degradation Properties of MgO Whiskers/PLLA Composite In Vitro.

Authors:  Yun Zhao; Bei Liu; Hongwei Bi; Jinjun Yang; Wei Li; Hui Liang; Yue Liang; Zhibin Jia; Shuxin Shi; Minfang Chen
Journal:  Int J Mol Sci       Date:  2018-09-13       Impact factor: 5.923

3.  Effects of Magnesium Oxide (MgO) Shapes on In Vitro and In Vivo Degradation Behaviors of PLA/MgO Composites in Long Term.

Authors:  Yun Zhao; Hui Liang; Shiqiang Zhang; Shengwei Qu; Yue Jiang; Minfang Chen
Journal:  Polymers (Basel)       Date:  2020-05-08       Impact factor: 4.329