Karina Kato Carneiro1, Marcia Margarete Meier2, Clenilton Costa Dos Santos3, Adeilton Pereira Maciel4, Ceci Nunes Carvalho5, José Bauer6.
Abstract
To evaluate the effect of incorporating niobium phosphate bioactive glass (NbG) into commercial etch-and-rinse adhesive systems, with and without silane, on their degree of conversion (DC) (%) and microtensile bond strength (μTBS). The NbG micro-filler was added to two etch-and-rinse adhesive systems: One Step (OS) and Prime & Bond (PB) at 40% concentration. The following groups were formed: control without glass addition OS; addition of unsilanized NbG (OSNbG); addition of silanized NbG (OSNbGS); control without glass PB; addition of unsilanized NbG (PBNbG); addition of silanized NbG (PBNbGS). The DC was determined using total Fourier spectroscopy reflection (FTIR/ATR). For μTBS testing, 48 human third molars (n=8) were restored and sliced to obtain specimens (0.8 mm2) and they were tested at two different time intervals: immediately and after 6 months. The fracture mode was evaluated with a stereoscopic loupe (40×) and by scanning electron microscopy (SEM). The data were subjected to ANOVA and Tukey tests (a=0.05). NbG addition did not compromise the adhesive system DC values (p>0.05). Furthermore, the NbG added to the adhesive systems did not affect μTBS values (p>0.05). Fracture occurred predominantly at the dentin-adhesive interface. NbG bioactive glass did not affect the DC or microtensile bond strength results.Entities:
Mesh:
Substances:
Year: 2016 PMID: 27982183 DOI: 10.1590/0103-6440201601110
Source DB: PubMed Journal: Braz Dent J ISSN: 0103-6440