| Literature DB >> 27853309 |
Jian Chen1, Xiaochan Xu1, Tao Li1, Kannusamy Pandiselvi1, Jingyu Wang1.
Abstract
Efficient metal-free visible photocatalysts with high stability are highly desired for sufficient utilization of solar energy. In this work, the popularEntities:
Year: 2016 PMID: 27853309 PMCID: PMC5112518 DOI: 10.1038/srep37318
Source DB: PubMed Journal: Sci Rep ISSN: 2045-2322 Impact factor: 4.379
Figure 1Schematic diagram for the synthesis of 2D/2D CNX-NSs/RGO hybrid.
Step I: structural modification approach; Step II: photo-assisted electrostatic assembly technique.
Figure 2XRD patterns of the samples.
Figure 3Raman spectra of graphite, GO, and CNX-NSs/RGO hybrid.
Figure 4TEM images of (a) bulk CNX and (b) exfoliated CNX-NSs sol catalysts. The inserts in b is the magnified TEM image. AFM images and the corresponding cross-sectional analysis of (c,d) CNX-NSs sol, (e,f) GO, and (g,h) CNX-NSs/RGO. (i) TEM image of CNX-NSs/RGO hybrid. (j) The magnified TEM image and (k-m) the corresponding elemental mapping images of CNX-NSs/RGO hybrid.
Figure 5FT-IR spectra of the as-prepared samples.
Figure 6The XPS survey spectra (a), high-resolution C1s spectra (b) high-resolution N1s spectra (c), and high-resolution O1s spectra (d) of GO, bulk CNX, exfoliated CNX-NSs, and CNX-NSs/RGO hybrid.
Figure 7UV-vis DRS of the samples (a) and Tauc Plot of (αhν)2 as a function of photon energy (hν) (b).
Figure 8Photoluminescence spectra of the as-prepared samples under 360 nm excitation.
Figure 9Photodegradation curve of MB dye over the prepared photocatalysts under full spectrum (a) and visible light (b) irradiation. (c) Nyquist plots of the as-prepared samples. (d) Photocurrent-time curves of as-prepared samples under visible light irradiation.
Figure 10Trapping test of photogenerated holes and radicals in CNX-NSs/RGO photodegradation system under visible-light irradiation.
(b) PL spectra for detection of H2O2 generation over different photocatalysts under 30 min visible light irradiation. The excitation wavelength is set as 290 nm.
Figure 11(a) LC data of photodegraded MB at given time intervals. (b,c) MS signals of the major detected intermediates eluting at 7.6 and 9.3 min.
Figure 12Comparison of possible photocatalytic mechanism of CNX-NSs (a) and the well-contacted 2D/2D CNX-NSs/RGO heterostructure (b) under visible light irradiation. (c) Possible degradation pathway from MB dye during photocatalytic reaction51.