Pure gutta-percha was heat-treated in a differential thermal analyzer. The high melting form crystallized on cooling when gutta-percha was heated to 70 C or less. Above 74 C, crystallization into the low melting form predominated. Either polymorph can be selectively crystallized by control of the heat-treatment temperature before cooling.Mesh: