| Literature DB >> 27238586 |
Abbas Teimouri1, Shima Ghanavati Nasab2, Niaz Vahdatpoor3, Saeed Habibollahi3, Hossein Salavati3, Alireza Najafi Chermahini4.
Abstract
In the present study, a series of chitosan/Zeolite Y/Nano Zirconium oxide (CTS/ZY/Nano ZrO2) nanocomposites were made by controlling the molar ratio of chitosan (CTS) to Zeolite Y/Nano Zirconium oxide in order to remove nitrate (NO3-) ions in the aqueous solution. The nanocomposite adsorbents were characterized by XRD, FTIR, BET, SEM and TEM. The influence of different molar ratios of CTS to ZY/Nano ZrO2, the initial pH value of the nitrate solution, contact time, temperature, the initial concentration of nitrate and adsorbent dose was studied. The adsorption isotherms and kinetics were also analyzed. It was attempted to describe the sorption processes by the Langmuir equation and the theoretical adsorption capacity (Q0) was found to be 23.58mg nitrate per g of the adsorbent. The optimal conditions for nitrate removal were found to be: molar ratio of CTS/ZY/Nano ZrO2: 5:1; pH: 3; 0.02g of adsorbent and temperature: 35°C, for 60min. The adsorption capacities of CTS, ZY, Nano ZrO2, CTS/Nano ZrO2, CTS/ZY and CTS/ZY/Nano ZrO2 nanocomposites for nitrate removal were compared, showing that the adsorption ability of CTS/ZY/Nano ZrO2 nanocomposite was higher than the average values of those of CTS (1.95mg/g for nitrate removal), ZY, Nano ZrO2, CTS/Nano ZrO2, and CTS/ZY.Entities:
Keywords: Adsorbent; Chitosan; Nano ZrO(2); Nanocomposite; Nitrate; Removal; Zeolite Y
Mesh:
Substances:
Year: 2016 PMID: 27238586 DOI: 10.1016/j.ijbiomac.2016.05.089
Source DB: PubMed Journal: Int J Biol Macromol ISSN: 0141-8130 Impact factor: 6.953