| Literature DB >> 2638848 |
Y Terada, S Maeyama, R Hirayasu.
Abstract
Gold and nickel-chromium alloys were used as substrates for one shade of fused porcelain. Chroma characteristics were compared between samples with opaque thicknesses of 0.1, 0.2, and 0.3 mm. Thicknesses of 0.1 to 0.5 mm of dentin porcelain fused on each of the thicknesses of opaque porcelain were measured. Perceptible color differences were found for most of the samples, and all nongold alloy samples showed such changes.Entities:
Mesh:
Substances:
Year: 1989 PMID: 2638848
Source DB: PubMed Journal: Int J Prosthodont ISSN: 0893-2174 Impact factor: 1.681