| Literature DB >> 26347345 |
Hyungwoo Kim1, Hemakesh Mohapatra1, Scott T Phillips2.
Abstract
Adhesives that selectively debond from a surface by stimuli-induced head-to-tail continuous depolymerization of poly(benzyl ether) macro-cross-linkers within a poly(norbornene) matrix are described. Continuous head-to-tail depolymerization provides faster rates of response than can be achieved using a small-molecule cross-linker, as well as responses to lower stimulus concentrations. Shear-stress values for glass held together by the adhesive reach 0.51±0.10 MPa, whereas signal-induced depolymerization via quinone methide intermediates reduces the shear stress values to 0.05±0.02 MPa. Changing the length of the macro-cross-linkers alters the time required for debonding, and thus enables the programmed sequential release of specific layers in a glass composite material.Entities:
Keywords: adhesives; depolymerization; materials science; polymers; stimuli-responsive materials
Year: 2015 PMID: 26347345 DOI: 10.1002/anie.201506511
Source DB: PubMed Journal: Angew Chem Int Ed Engl ISSN: 1433-7851 Impact factor: 15.336