The Effect of Hydrofluoric Acid Concentration on the Bond Strength and Morphology of the Surface and Interface of Glass Ceramics to a Resin Cement.

D Sundfeld Neto, L Z Naves, A R Costa, A B Correr, S Consani, G A Borges, L Correr-Sobrinho.   

Abstract

The purpose of this study was to evaluate the influence of various concentrations of hydrofluoric acid (HF) on the surface/interface morphology and μ-shear bond strength (μSBS) between IPS Empress Esthetic (EST) (Ivoclar Vivadent) and IPS e.max Press (EMX) (Ivoclar Vivadent) ceramics and resin cement. Ceramic blocks were divided into 12 groups for each kind of ceramic. Six different HF concentrations were evaluated: 1%, 2.5%, 5%, 7.5%, 10%, and 15%. All groups were silanated after etching, and half of the specimens within each group received a thin layer of unfilled resin (UR). Three resin cement cylinders were prepared on each ceramic block for μSBS testing. The specimens were stored in distilled water at 37°C for 24 hours. The μSBS test was carried out in a universal testing machine at a crosshead speed of 0.5 mm/min until fracture. The data were submitted to three-way analysis of variance and multiple comparisons were performed using the Tukey post hoc test (p<0.05). The etched surfaces and bonded interfaces were evaluated using scanning electron microscopy. μSBS means (MPa) for 1%, 2.5%, 5%, 7.5%, 10%, and 15% HF concentrations were, respectively, 25.2, 27.2, 30.1, 31.4, 33.3, and 31.8. μSBS means with or without UR application measured 32.24 and 27.4, respectively; EST and EMX measured 29.8 and 29.9, respectively. For the HF concentrations, 10% and 15% showed higher μSBS means than did 1% and 2.5% (p<0.05); 7.5% was higher than 1% (p<0.05); and no statistical differences were found among the other concentrations (p>0.05). When evaluating UR, μSBS mean was significantly higher and better infiltration was observed on the etched surfaces. No statistical difference was found between the ceramics. The HF concentration and UR influenced the bond strength and surface/interface morphology.

Entities:  

Mesh:

Substances:

Year:  2015        PMID: 25764043     DOI: 10.2341/14-133-L

Source DB:  PubMed          Journal:  Oper Dent        ISSN: 0361-7734            Impact factor:   2.440


  10 in total

1.  Bond strength of lithium disilicate after cleaning methods of the remaining hydrofluoric acid.

Authors:  Daniela-Micheline Dos Santos; Sandro-Basso Bitencourt; Emily-Vivianne-Freitas da Silva; Adaias-Oliveira Matos; Georgia-de Castro Benez; Elidiane-Cipriano Rangel; Aldiéris-Alves Pesqueira; Valentim-Adelino-Ricardo Barão; Marcelo-Coelho Goiato
Journal:  J Clin Exp Dent       Date:  2020-02-01

2.  Bonding of Clear Aligner Composite Attachments to Ceramic Materials: An In Vitro Study.

Authors:  Bashair A Alsaud; Maher S Hajjaj; Ahmad I Masoud; Ensanya A Abou Neel; Dalia A Abuelenain; Amal I Linjawi
Journal:  Materials (Basel)       Date:  2022-06-10       Impact factor: 3.748

3.  Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading.

Authors:  Leyla Sadighpour; Farideh Geramipanah; Vanya Rasaei; Mohammad J Kharazi Fard
Journal:  Int J Dent       Date:  2018-04-17

4.  HF etching of CAD/CAM materials: influence of HF concentration and etching time on shear bond strength.

Authors:  Antonio Straface; Lena Rupp; Aiste Gintaute; Jens Fischer; Nicola U Zitzmann; Nadja Rohr
Journal:  Head Face Med       Date:  2019-08-08       Impact factor: 2.151

5.  Interaction of a universal adhesive with different surface treatments with feldespathic ceramics.

Authors:  Diana Alejandra Suárez-Moya; Alberto Carlos Cruz-González; Juan Norberto Calvo-Ramírez
Journal:  Saudi Dent J       Date:  2019-03-25

6.  Effect of experimental resin cements containing thio-urethane oligomers on the durability of ceramic-composite bonded interfaces.

Authors:  Lourenço Correr-Sobrinho; Ana Rosa Costa; Ana Paula P Fugolin; Daniel Sundfeld Neto; Jack L Ferracane; Carmem S Pfeifer
Journal:  Biomater Investig Dent       Date:  2019-11-27

7.  Surface Treatment Effect on Shear Bond Strength between Lithium Disilicate Glass-Ceramic and Resin Cement.

Authors:  Siripan Simasetha; Awiruth Klaisiri; Tool Sriamporn; Kraisorn Sappayatosok; Niyom Thamrongananskul
Journal:  Eur J Dent       Date:  2021-12-17

8.  Effect of Surface Coating on Bond Strength between Etched Feldspar Ceramic and Resin-Based Luting Agents.

Authors:  Jader Sebben; Volni A Canevese; Rodrigo Alessandretti; Gabriel K R Pereira; Rafael Sarkis-Onofre; Ataís Bacchi; Aloísio O Spazzin
Journal:  Biomed Res Int       Date:  2018-07-24       Impact factor: 3.411

9.  Effect of Die Spacer Thickness on the Microshear Bond Strength of CAD/CAM Lithium Disilicate Veneers.

Authors:  Sherine Mohamed Farag; Mona Mohamed Ghoneim; Rania Reda Afifi
Journal:  Int J Dent       Date:  2021-07-23

10.  Effect of lithium disilicate ceramic thickness, shade and translucency on transmitted irradiance and knoop microhardness of a light cured luting resin cement.

Authors:  Lincoln Pires Silva Borges; Gilberto Antônio Borges; Américo Bortolazzo Correr; Jeffrey A Platt; Sidney Kina; Lourenço Correr-Sobrinho; Ana Rosa Costa
Journal:  J Mater Sci Mater Med       Date:  2021-07-31       Impact factor: 3.896

  10 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.