After base treatment of ZSM-5 crystals below 100 nm in size, TEM shows hollow single crystals with a 10 nm shell. SEM images confirm that the shell is well- preserved even after prolonged treatment. Determination of the Si/Al ratios with AAS and XPS in combination with argon sputtering reveals aluminum zoning of the parent zeolite, and the total pore volume increases in the first two hours of base treatment. In corresponding TEM images, the amount of hollow crystals are observed to increase during the first two hours of base treatment, and intact crystals are visible even after 10 h of leaching; these observations indicate different dissolution rates between individual crystals. TEM of large, commercially available ZSM-5 crystals shows inhomogeneous distribution of mesopores among different crystals, which points to the existence of structural differences between individual crystals. Only tetrahedrally coordinated aluminum is detected with (27) Al MAS NMR after the base leaching of nano-sized ZSM-5.
© 2015 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Entities:  

Keywords:  ZSM-5; aluminum; base leaching; desilication; zeolites

Year:  2015        PMID: 25720305     DOI: 10.1002/chem.201406182

Source DB:  PubMed          Journal:  Chemistry        ISSN: 0947-6539            Impact factor:   5.236


  4 in total

1.  X-ray Excited Optical Fluorescence and Diffraction Imaging of Reactivity and Crystallinity in a Zeolite Crystal: Crystallography and Molecular Spectroscopy in One.

Authors:  Zoran Ristanović; Jan P Hofmann; Marie-Ingrid Richard; Tao Jiang; Gilbert A Chahine; Tobias U Schülli; Florian Meirer; Bert M Weckhuysen
Journal:  Angew Chem Weinheim Bergstr Ger       Date:  2016-05-04

2.  Single Molecule Nanospectroscopy Visualizes Proton-Transfer Processes within a Zeolite Crystal.

Authors:  Zoran Ristanović; Alexey V Kubarev; Johan Hofkens; Maarten B J Roeffaers; Bert M Weckhuysen
Journal:  J Am Chem Soc       Date:  2016-10-06       Impact factor: 15.419

3.  Nanoscale tomography reveals the deactivation of automotive copper-exchanged zeolite catalysts.

Authors:  Joel E Schmidt; Ramon Oord; Wei Guo; Jonathan D Poplawsky; Bert M Weckhuysen
Journal:  Nat Commun       Date:  2017-11-21       Impact factor: 14.919

4.  X-ray Excited Optical Fluorescence and Diffraction Imaging of Reactivity and Crystallinity in a Zeolite Crystal: Crystallography and Molecular Spectroscopy in One.

Authors:  Zoran Ristanović; Jan P Hofmann; Marie-Ingrid Richard; Tao Jiang; Gilbert A Chahine; Tobias U Schülli; Florian Meirer; Bert M Weckhuysen
Journal:  Angew Chem Int Ed Engl       Date:  2016-05-04       Impact factor: 15.336

  4 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.