Y Lu1, A R Bradshaw1, Y L Chiu1, I P Jones1.
Abstract
The bio-corrosion behaviour of Mg-3Zn-0.3Ca (wt.%) alloy in simulated body fluid (SBF) at 37°C has been investigated using immersion testing and electrochemical measurements. Heat treatment has been used to alter the grain size and secondary phase volume fraction; the effects of these on the bio-corrosion behaviour of the alloy were then determined. The as-cast sample has the highest bio-corrosion rate due to micro-galvanic corrosion between the eutectic product (Mg+Ca2Mg6Zn3) and the surrounding magnesium matrix. The bio-corrosion resistance of the alloy can be improved by heat treatment. The volume fraction of secondary phases and grain size are both key factors controlling the bio-corrosion rate of the alloy. The bio-corrosion rate increases with volume fraction of secondary phase. When this is lower than 0.8%, the dependence of bio-corrosion rate becomes noticeable: large grains corrode more quickly.Entities:
Keywords: Degradation; Heat treatment; Mg–Zn–Ca; Microstructure
Mesh:
Substances:
Year: 2014 PMID: 25579949 DOI: 10.1016/j.msec.2014.12.049
Source DB: PubMed Journal: Mater Sci Eng C Mater Biol Appl ISSN: 0928-4931 Impact factor: 7.328