| Literature DB >> 25439895 |
Ran Li1, Meng He1, Tong Li1, Lina Zhang2.
Abstract
We prepared cellulose/silver nanocomposite fibers by soaking the cellulose fibers in AgNO3 aqueous solution, which was heated at 80°C for 24h to synthesize Ag nanoparticles in situ. The structure and properties of the composite fibers were characterized by FT-IR, X-ray diffraction (XRD), scanning electron microscopy (SEM), transmitting electron microscopy (TEM), thermo-gravimetric analysis (TGA) and tensile testing. The content and diameter of the Ag nanoparticles (NPs) increased from 0.15% to 2.40% and from 7.2 nm to 12.5 nm, respectively. In our findings, the pores of the cellulose fiber at wet state were used as a microreactor to synthesize Ag nanopariticles. The cellulose/Ag nanocomposite fibers exhibited good mechanical properties and thermal stability. Antibacterial experiment revealed excellent antibacterial activity of the cellulose nanocomposite fibers against Staphylococcus aureus. The cellulose/silver nanocomposite fibers would have great potential in antibacterial textile and wound handling due to easy industrialization.Entities:
Keywords: Antibacterial; Cellulose fiber; Hydrothermal reduction; Silver nanoparticles
Mesh:
Substances:
Year: 2014 PMID: 25439895 DOI: 10.1016/j.carbpol.2014.08.046
Source DB: PubMed Journal: Carbohydr Polym ISSN: 0144-8617 Impact factor: 9.381