Reduced UHMWPE wear using magnesia-stabilized zirconia instead of CoCr femoral components in a knee simulator.

Marcel E Roy1, Leo A Whiteside2, David S Tilden3, Oscar F Noel4.   

Abstract

Magnesia-stabilized zirconia (Mg-PSZ) is stable and maintains a scratch-resistant surface in hip replacement, but is untested in knees. We assessed whether using Mg-PSZ instead of cobalt-chromium (CoCr) femoral components resulted in less tibial insert wear, and evaluated changes in topography and roughness of the femoral components. Inserts bearing against CoCr or Mg-PSZ were tested using standard (9 Mc) and aggressive (6 Mc) waveforms. Femoral component surface topography and roughness were evaluated before and after testing by optical profilometry. When bearing against Mg-PSZ, UHMWPE wear rate decreased by 73% (standard) and by 59% (aggressive conditions). After 15 Mc, CoCr components featured deep scratches, and roughness increased five-fold, while Mg-PSZ components were unchanged. Mg-PSZ femoral components may be indicated for high-demand patients and those with metal sensitivity.
Copyright © 2014 Elsevier Inc. All rights reserved.

Entities:  

Keywords:  ceramic; cobalt chromium; roughness; total knee arthroplasty; wear

Mesh:

Substances:

Year:  2014        PMID: 25316377     DOI: 10.1016/j.arth.2014.09.027

Source DB:  PubMed          Journal:  J Arthroplasty        ISSN: 0883-5403            Impact factor:   4.757


  1 in total

1.  Wear Performance of Calcium Carbonate-Containing Knee Spacers.

Authors:  Ulrike Mueller; Joern Reinders; Sydney Smith-Romanski; Jan Philippe Kretzer
Journal:  Materials (Basel)       Date:  2017-07-15       Impact factor: 3.623

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.