Shuqiong Liu1, Zhihang He2, Guojie Xu2, Xiufeng Xiao3.
Abstract
Three-dimensional polycaprolactone (PCL) scaffolds with spherulite and nanofibrous structures were fabricated for the first time by thermally induced phase separation from a ternary PCL/dioxane/water system. Moreover, the effects of polymer concentration, aging temperature and the ratio of dioxane to water on the morphology of nanofibrous scaffolds were investigated. The result revealed that gelation, aging temperature, and ratio of solvents significantly influenced the formation of the unique spherulite and nanofibrous structures. The apatite-formation ability test showed relatively rapid growth of carbonate hydroxyapatite in the nanofibrous PCL scaffold with macropore compared to the other two scaffolds with smooth structure and nanofibrous structure without macropore, respectively, indicating good apatite-formation ability of the macroporous and nanofibrous PCL scaffolds.Entities:
Keywords: Nanofibrous; Phase separation; Polycaprolactone; Spherulite
Mesh:
Substances:
Year: 2014 PMID: 25280697 DOI: 10.1016/j.msec.2014.08.012
Source DB: PubMed Journal: Mater Sci Eng C Mater Biol Appl ISSN: 0928-4931 Impact factor: 7.328