Literature DB >> 25137055

Synthesis, PL characterizations and concentration quenching effect in Dy(3+) and Eu(3+) activated LiCaBO3 phosphor.

V R Kharabe1, Abha H Oza, S J Dhoble.   

Abstract

LiCaBO3 :Dy(3+) /Eu(3+) phosphors were synthesized by a solid-state reaction. The synthesized materials were characterized using powder X-ray diffraction pattern (XRD) for confirmation. All the structural parameters were calculated from the XRD data. Scanning electron microscopy (SEM) images showed rod-like morphology. Photoluminescence (PL) emission spectra showed two emissions (484 and 577 nm) in Dy(3+) -doped LiCaBO3 :Dy(3+) phosphors with the concentration quenching effect and the critical distance was calculated to be about 22.76 Å. LiCaBO3 :Eu(3+) phosphor was effectively excited by a near-UV light of 392 nm. The emission spectra exhibited the transition from (5) D0 level to (7) FJ (J = 0-2) with main emission at 614 nm, which comes from the electrodipole transition because of the asymmetric point group. The quenching concentration of Eu(3+) is about 0.2 mol%, and the critical distance was calculated to be about 38.93 Å.
Copyright © 2014 John Wiley & Sons, Ltd.

Keywords:  PL emission; concentration quenching; critical distance; solid-state reaction

Mesh:

Substances:

Year:  2014        PMID: 25137055     DOI: 10.1002/bio.2756

Source DB:  PubMed          Journal:  Luminescence        ISSN: 1522-7235            Impact factor:   2.464


  1 in total

1.  Barium molybdate white emitting phosphor synthesized at room temperature by co-precipitation.

Authors:  Soung-Soo Yi; Jae-Yong Jung
Journal:  RSC Adv       Date:  2022-08-08       Impact factor: 4.036

  1 in total