Eun Ji Park1, Youn Kyoung Cho, Dae Han Kim, Myung-Geun Jeong, Yong Ho Kim, Young Dok Kim.
Abstract
Mesoporous silica with mean pore size of ∼14 nm was coated by polydimethylsiloxane (PDMS) using a thermal deposition method. We showed that the inner walls of pores larger than ∼8 nm can be coated by thin layers of PDMS, and the surfaces consisting of PDMS-coated silica were superhydrophobic, with water contact angles close to 170°. We used the PDMS-coated silica as adsorbents of various gas-phase chemical warfare agent (CWA) simulants. PDMS-coated silica allowed molecular desorption of various CWA simulants even after exposure under highly humid conditions and, therefore, is applicable as an agent for the preconcentration of gas-phase analytes to enhance the sensitivities of various sensors.Entities:
Year: 2014 PMID: 25102134 DOI: 10.1021/la502915r