| Literature DB >> 25024836 |
Sogra Yassaei1, Reza Fekrazad2, Neda Shahraki3, Mahdjoube Goldani Moghadam4.
Abstract
Background and aims. The aim of this study was to compare shear bond strength (SBS) of metal and ceramic brackets bonded to enamel using acid versus Er:YAG laser etching. Materials and methods. Eighty premolars were divided into 4 groups: AM (acid etching/ metal brackets), AC (acid etching/ ceramic brackets), LM (laser etching/ metal brackets) and LC (laser etching/ ceramic brackets). Enamel condition-ing was done using acid in AC and AM and Er:YAG laser in LC and LM. Brackets were debonded with a Dartec machine and the SBSs were determined. Adhesive remnant index was evaluated under a stereomicroscope. Two additional teeth were conditioned with acid and laser for scanning electron microscopy examination. Comparisons of SBS value were done by ANOVA test. Results. statistical analyses showed that SBSs of acid groups were significantly higher than that of laser groups, but dif-ferences between SBS values of AC/ AM and LC/LM were not significant. SEM examination revealed different etching pattern. Conclusion. Low power Er:YAG laser etching offers clinically acceptable SBS which besides its other superiorities to acid etching can be an appropriate alternative for bonding of ceramic brackets.Entities:
Keywords: Er:YAG laser; etching, laser; orthodontic
Year: 2014 PMID: 25024836 PMCID: PMC4091696 DOI: 10.5681/joddd.2014.005
Source DB: PubMed Journal: J Dent Res Dent Clin Dent Prospects ISSN: 2008-210X