Fracture resistance of a selection of full-contour all-ceramic crowns: an in vitro study.

Tim F Zesewitz, Andreas W Knauber, Frank P Nothdurft.   

Abstract

This study aimed to evaluate the fracture resistance of monolithic single crowns made from zirconia (ZI), lithium disilicate (LS2), or feldspar ceramic (FC). Five groups of crowns representing a maxillary first molar were made with the appropriate dimensions according to the manufacturer's instructions. The ZI and LS2 crowns were luted adhesively or cemented conventionally on a metal abutment tooth analog. The feldspar ceramic crowns were luted adhesively. All specimens underwent axial loading until fracture. The crowns in the ZI groups possessed the highest fracture resistance independent of the mode of fixation.

Entities:  

Mesh:

Substances:

Year:  2014        PMID: 24905268     DOI: 10.11607/ijp.3815

Source DB:  PubMed          Journal:  Int J Prosthodont        ISSN: 0893-2174            Impact factor:   1.681


  13 in total

1.  Choice of cement for single-unit crowns: Findings from The National Dental Practice-Based Research Network.

Authors:  Nathaniel C Lawson; Mark S Litaker; Jack L Ferracane; Valeria V Gordan; Alan M Atlas; Tara Rios; Gregg H Gilbert; Michael S McCracken
Journal:  J Am Dent Assoc       Date:  2019-04-25       Impact factor: 3.634

2.  Effect of Surface Treatment and Cement on Fracture Load of Traditional Zirconia (3Y), Translucent Zirconia (5Y), and Lithium Disilicate Crowns.

Authors:  Nathaniel C Lawson; Carlos A Jurado; Chan-Te Huang; Geoffrey P Morris; John O Burgess; Perng-Ru Liu; Keith E Kinderknecht; Chee Paul Lin; Daniel A Givan
Journal:  J Prosthodont       Date:  2019-06-11       Impact factor: 2.752

3.  Fracture-resistant monolithic dental crowns.

Authors:  Yu Zhang; Zhisong Mai; Amir Barani; Mark Bush; Brian Lawn
Journal:  Dent Mater       Date:  2016-01-11       Impact factor: 5.304

4.  In vitro performance and fracture resistance of CAD/CAM-fabricated implant supported molar crowns.

Authors:  Martin Rosentritt; Sebastian Hahnel; Frank Engelhardt; Michael Behr; Verena Preis
Journal:  Clin Oral Investig       Date:  2016-07-01       Impact factor: 3.573

5.  Load-bearing capacity of various CAD/CAM monolithic molar crowns under recommended occlusal thickness and reduced occlusal thickness conditions.

Authors:  Sulki Choi; Hyung-In Yoon; Eun-Jin Park
Journal:  J Adv Prosthodont       Date:  2017-12-14       Impact factor: 1.904

6.  Wear Behavior of Ceramic CAD/CAM Crowns and Natural Antagonists.

Authors:  Ella A Naumova; Stephan Schneider; Wolfgang H Arnold; Andree Piwowarczyk
Journal:  Materials (Basel)       Date:  2017-02-28       Impact factor: 3.623

7.  Fracture resistance of implant- supported monolithic crowns cemented to zirconia hybrid-abutments: zirconia-based crowns vs. lithium disilicate crowns.

Authors:  Shareen H Elshiyab; Noor Nawafleh; Andreas Öchsner; Roy George
Journal:  J Adv Prosthodont       Date:  2018-02-12       Impact factor: 1.904

8.  The Effect of Sintering Program on the Compressive Strength of Zirconia Copings.

Authors:  Amir Ali Reza Khaledi; Mahroo Vojdani; Mitra Farzin; Soudabeh Pirouzi
Journal:  J Dent (Shiraz)       Date:  2018-09

9.  Effect of cements on fracture resistance of monolithic zirconia crowns.

Authors:  Keisuke Nakamura; Mathieu Mouhat; John Magnus Nergård; Solveig Jenssen Lægreid; Taro Kanno; Percy Milleding; Ulf Örtengren
Journal:  Acta Biomater Odontol Scand       Date:  2016-01-26

10.  Fatigue Fracture Strength of Implant-Supported Full Contour Zirconia and Metal Ceramic Fixed Partial Dentures.

Authors:  Fariborz Vafaee; Farnaz Firouz; Masoumeh Khoshhal; Amirarsalan Hooshyarfard; Armaghan Shahbazi; Ghodratollah Roshanaei
Journal:  J Dent (Tehran)       Date:  2017-05
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.