K Raja1, P S Ramesh2, D Geetha1.
Abstract
An investigation on Fe-doped ZnO (Zn1-xFexO, x=0, 0.03, 0.06 and 0.09mM) nanopowder have been synthesized by co-precipitated method annealed at 550°C were reported. The structural, morphological and optical properties of the samples were studied by X-ray diffraction (XRD), scanning electron microscopy (SEM) with energy dispersive spectra (EDS) analysis, Atomic Force Microscopy (AFM), UV-Visible spectroscopy, and photoluminescence (PL) techniques, Fourier transform infrared (FTIR) spectroscopy. The XRD spectrum shows all the samples are hexagonal wurtzite structure. The presence of functional groups and chemical bonding are confirmed by FT-IR. The PL spectra of the Zn1-xFexxO systems show that the shift in near band edge (NBE) UV emission from 344.54 to 364.21nm and a shift in green band (GB) emission from 484 to 540nm which conforms the substitution of Fe into the ZnO lattice. UV-Visible measurement showed a decrease in the energy gap with increasing Fe content, probably due to an increase in the lattice parameters. It is also found that these results are in good agreement with other calculated and experimental results.Entities:
Keywords: Fourier transform infrared spectroscopy; Optical band gap; UV–Visible spectroscopy
Mesh:
Substances:
Year: 2014 PMID: 24835724 DOI: 10.1016/j.saa.2014.03.047
Source DB: PubMed Journal: Spectrochim Acta A Mol Biomol Spectrosc ISSN: 1386-1425 Impact factor: 4.098