In this study, chitosan-PEO blend, prepared in a 15 M acetic acid, was electrospun into nanofibers (~78 nm diameter) with bead free morphology. While investigating physico-chemical parameters of blend solutions, effect of yield stress on chitosan based nanofiber fabrication was clearly evidenced. Architectural stability of nanofiber mat in aqueous medium was achieved by ionotropic cross-linking of chitosan by tripolyphosphate (TPP) ions. The TPP cross-linked nanofiber mat showed swelling up to ~300% in 1 h and ~40% degradation during 30 day study period. 3T3 fibroblast cells showed good attachment, proliferation and viability on TPP treated chitosan based nanofiber mats. The results indicate non-toxic nature of TPP cross-linked chitosan based nanofibers and their potential to be explored as a tissue engineering matrix.Entities:
Keywords: Chitosan; Cytocompatibility; Electrospinning; Tripolyphosphate; Yield stress
Mesh:
Substances:
Year: 2012 PMID: 23827594 DOI: 10.1016/j.msec.2012.12.066
Source DB: PubMed Journal: Mater Sci Eng C Mater Biol Appl ISSN: 0928-4931 Impact factor: 7.328