| Literature DB >> 23033259 |
Peter Jakes1, Gil Cohn, Yair Ein-Eli, Frieder Scheiba, Helmut Ehrenberg, Rüdiger-A Eichel.
Abstract
The electrocatalytical process at the air cathode in novel silicon-air batteries using the room-temperature ionic liquid hydrophilic 1-ethyl-3-methylimidazolium oligofluorohydrogenate [EMI⋅2.3 HF⋅F] as electrolyte and highly doped silicon wafers as anodes is investigated by electrochemical means, X-ray photoelectron spectroscopy (XPS), and electron paramagnetic resonance (EPR) spectroscopy. The results obtained by XPS and EPR provide a model to describe the limited discharge capacity by means of a mechanism of air-electrode deactivation. In that respect, upon discharge the silicon-air battery's cathode is not only blocked by silicon oxide reduction products, but also experiences a major modification in the MnO₂ catalyst nature. The proposed modification of the MnO₂ catalyst by means of a MnF₂ surface layer greatly impacts the Si-air performance and describes a mechanism relevant for other metal-air batteries, such as the lithium-air. Moreover, the ability for this deactivation layer to form is greatly impacted by water in the electrolyte.Entities:
Mesh:
Substances:
Year: 2012 PMID: 23033259 DOI: 10.1002/cssc.201200199
Source DB: PubMed Journal: ChemSusChem ISSN: 1864-5631 Impact factor: 8.928