Solar active fire clay based hetero-Fenton catalyst over a wide pH range for degradation of Acid Violet 7.

Inbasekaran Muthuvel1, Balu Krishnakumar, Meenakshisundaram Swaminathan.   

Abstract

Fe(III) immobilized fire clay (Fe-FC) was prepared using ferric nitrate by solid state dispersion method and this hetero-Fenton catalyst was applied for the degradation of Acid Violet 7 (AV 7) under natural sunlight. The 26% ferric nitrate loaded fire clay was found to be most efficient. The experimental conditions such as solution pH, H2O2 concentration for efficient degradation of AV 7 have been determined. Unlike Fenton catalyst, Fe-FC is photoactive over a wide pH range of 3-7. This catalyst was found to be stable and reusable. The GC-MS analysis of experimental solutions during irradiation revealed the formation of 2,8-diaminonaphthalene-1,3,6-triol, 8-aminonaphthalene-1,2,3,6-tetrol, 2-aminonaphthalene-1,3,6,8-tetrol and 2-aminobenzene-1,3-diol/5-aminonbenzene-1,3-diol/ 2-aminobenzene-1,4-diol as intermediates. The 26% ferric nitrate loaded fire clay was characterized by XRD, ICP-AES, BET surface area, FT-IR, SEM-EDS and UV-DRS studies.

Entities:  

Mesh:

Substances:

Year:  2012        PMID: 22655369     DOI: 10.1016/s1001-0742(11)60754-7

Source DB:  PubMed          Journal:  J Environ Sci (China)        ISSN: 1001-0742            Impact factor:   5.565


  1 in total

1.  Phenol degradation using the mixed material clay/Fe immobilized on glass slides.

Authors:  Lidiane Yumi Taketa; Franciély Ignachewski; Juan Carlo Villalba; Fauze Jacó Anaissi; Sérgio Toshio Fujiwara
Journal:  Environ Sci Pollut Res Int       Date:  2014-07-29       Impact factor: 4.223

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.