Abstract

OBJECTIVES: To determine the degree of conversion (DC) and Knoop microhardness (KHN) of resin-based composites (RBCs) containing trimethylbenzoyl-diphenylphosphine oxide (TPO) cured by polywave or monowave LED light-curing units (LCUs).
METHODS: Three groups (each n = 5) of Tetric EvoCeram (Ivoclar Vivadent), Vit-l-escence (Ultradent) and Herculite XRV Ultra (Kerr) were prepared in Teflon moulds (5mm in diameter and 2mm thick) and cured with polywave Bluephase(®) G2 (Ivoclar Vivadent), polywave Valo (Ultradent) or monowave Bluephase(®) (Ivoclar Vivadent; control) resulting in 9 groups. DC and KHN were determined using micro-Raman spectroscopy and Knoop microhardness, respectively. High-performance liquid chromatography and nuclear magnetic resonance spectroscopy were used to confirm the presence or absence of TPO in the three uncured materials. Data were statistically analysed using two-way and one-way ANOVA and DC and KHN were correlated using Pearson's correlation (α = 0.05).
RESULTS: TPO was confirmed in Tetric EvoCeram and Vit-l-escence but not in Herculite XRV Ultra. All three LCUs produced comparable KHN for Tetric EvoCeram and Herculite XRV Ultra (p > 0.05). Both polywave LCUs resulted in significantly higher KHN for Vit-l-escence and higher DC in Tetric EvoCeram and Vit-l-escence than the monowave Bluephase(®) (p < 0.05). Conversely, Bluephase(®) showed higher DC than the two polywave LCUs in Herculite XRV Ultra (p < 0.05). Pearson's correlation coefficient was r = 0.818.
CONCLUSIONS: Polywave LED LCUs improved monomer to polymer conversion and KHN in the two TPO-containing RBCs, but not in Herculite XRV Ultra. DC and KHN were linearly correlated in all three RBCs. Vit-l-escence showed the highest DC and KHN of the three materials tested. CLINICAL SIGNIFICANCE: The use of polywave LEDs significantly improves both the DC and KHN of materials which contain TPO. This should be taken into account when curing bleached shades of RBCs even if the manufacturers do not indicate the presence of TPO in their materials.
Copyright © 2012 Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2012        PMID: 22465876     DOI: 10.1016/j.jdent.2012.03.007

Source DB:  PubMed          Journal:  J Dent        ISSN: 0300-5712            Impact factor:   4.379


  14 in total

1.  Effect of two lasers on the polymerization of composite resins: single vs combination.

Authors:  Jung-Hoon Ro; Sung-Ae Son; Jeong-kil Park; Gye-Rok Jeon; Ching-Chang Ko; Yong Hoon Kwon
Journal:  Lasers Med Sci       Date:  2015-04-17       Impact factor: 3.161

2.  Effect of 457 nm diode-pumped solid state laser on the polymerization composite resins: microhardness, cross-link density, and polymerization shrinkage.

Authors:  Sung-Ae Son; Jeong-Kil Park; Kyoung-Hwa Jung; Ching-Chang Ko; Chang-Mo Jeong; Yong Hoon Kwon
Journal:  Photomed Laser Surg       Date:  2014-12-30       Impact factor: 2.796

3.  The effects of extended curing time and radiant energy on microhardness and temperature rise of conventional and bulk-fill resin composites.

Authors:  Matej Par; Igor Repusic; Hrvoje Skenderovic; Ognjen Milat; Jelena Spajic; Zrinka Tarle
Journal:  Clin Oral Investig       Date:  2019-01-28       Impact factor: 3.573

4.  Polymerization pattern characterization within a resin-based composite cured using different curing units at two distances.

Authors:  Afnan O Al-Zain; George J Eckert; Henry Lukic; Spiro Megremis; Jeffrey A Platt
Journal:  Clin Oral Investig       Date:  2019-02-09       Impact factor: 3.573

5.  Clinical long-term success of contemporary nano-filled resin composites in class I and II restorations cured by LED or halogen light.

Authors:  Torsten Pflaum; Stefan Kranz; Regina Montag; Arndt Güntsch; Andrea Völpel; Robin Mills; Klaus Jandt; Bernd Sigusch
Journal:  Clin Oral Investig       Date:  2017-10-28       Impact factor: 3.573

6.  Curing effectiveness of single-peak and multi-peak led light curing units on tpo-containing resin composites with different chromatic characteristics.

Authors:  G Conte; M Panetta; M Mancini; A Fabianelli; A Brotzu; R Sorge; L Cianconi
Journal:  Oral Implantol (Rome)       Date:  2017-09-27

7.  Curing characteristics of flowable and sculptable bulk-fill composites.

Authors:  Vesna Miletic; Pong Pongprueksa; Jan De Munck; Neil R Brooks; Bart Van Meerbeek
Journal:  Clin Oral Investig       Date:  2016-07-06       Impact factor: 3.573

8.  Comparative study of surface microhardness of methacrylate-based composite resins polymerized with light-emitting diodes and halogen.

Authors:  Camila Sabatini
Journal:  Eur J Dent       Date:  2013-07

9.  Effects of radiant exposure and wavelength spectrum of light-curing units on chemical and physical properties of resin cements.

Authors:  Adriano Fonseca Lima; Stephanie Ellen Ferreira Formaggio; Lígia França Aires Zambelli; Alan Rodrigo Muniz Palialol; Giselle Maria Marchi; Cintia Helena Coury Saraceni; Marcelo Tavares de Oliveira
Journal:  Restor Dent Endod       Date:  2016-09-26

10.  Effects of delivering the same radiant exposures at 730, 1450, and 2920 mW/cm2 to two resin-based composites.

Authors:  Maan M AlShaafi
Journal:  Eur J Dent       Date:  2017 Jan-Mar
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.