Two-body wear resistance of some indirect composite resins.

Omid Savabi1, Farahnaz Nejatidanesh, Mitra Shabanian, Zahra Anbari.   

Abstract

The aim of this study was to evaluate two-body wear of five indirect composites and compare them with enamel. Signum, belleGlass HP, SR Adoro, Dialog, GC Gradia and enamel were formed into cylinders (n = 10). Two-body abrasive wear rates were determined using a porcelain disk and a pin on disk apparatus. The height and weight loss of the specimens were measured by stereomicroscope and digital scale. The data were subjected to analysis of variance and Tukey HSD tests to determine significant differences (alpha = 0.05). GC Gradia showed significantly less wear resistance than the other materials. Enamel was more resistant than any of the tested composites. Within the limitations of this study it can be concluded that the type of resin, filler size and method of polymerization could have affect the two-body abrasion resistance of indirect composites.

Entities:  

Mesh:

Substances:

Year:  2011        PMID: 21780731

Source DB:  PubMed          Journal:  Eur J Prosthodont Restor Dent        ISSN: 0965-7452


  1 in total

1.  Effect of two prophylaxis methods on marginal gap of Cl Vresin-modified glass-ionomer restorations.

Authors:  Soodabeh Kimyai; Fatemeh Pournaghi-Azar; Mehdi Daneshpooy; Mehdi Abed Kahnamoii; Farnaz Davoodi
Journal:  J Dent Res Dent Clin Dent Prospects       Date:  2016-03-16
  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.