Cellulose extraction from wood chip in an ionic liquid 1-allyl-3-methylimidazolium chloride (AmimCl).

Xuejing Wang1, Huiquan Li, Yan Cao, Qing Tang.   

Abstract

In the present study, 1-allyl-3-methylimidazolium chloride (AmimCl), an ionic liquid (IL), was used to extract cellulose from pine, poplar, Chinese parasol, and catalpa wood chips. Results show that pine is the most suitable wood species for cellulose extraction with ILs. Its cellulose extraction rate can reach as high as 62% under optimized conditions and its cellulose content is as high as 85% when DMSO/water is used as the precipitant. The dissolution process can be clearly observed by hot stage optical microscopy, and the reaction time can be significantly reduced by microwave irradiation. (13)C CP/MAS NMR, FTIR, XRD, and SEM were used to analyze the cellulose-rich extracts of pine. Results show that IL dissolves pine wood by destroying inter and intramolecular hydrogen bonds between lignocelluloses. The major component of pine extract is cellulose with a homogeneous and dense structure. After extraction, AmimCl can be easily recycled and reused.
Copyright © 2011 Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2011        PMID: 21684735     DOI: 10.1016/j.biortech.2011.05.064

Source DB:  PubMed          Journal:  Bioresour Technol        ISSN: 0960-8524            Impact factor:   9.642


  3 in total

Review 1.  Recent advances in 3D printing of nanocellulose: structure, preparation, and application prospects.

Authors:  Liang Ying Ee; Sam Fong Yau Li
Journal:  Nanoscale Adv       Date:  2020-12-28

2.  Synthesis and application of cationised cellulose for removal of Cr(VI) from acid mine-drainage contaminated water.

Authors:  Anita Etale; Dineo S Nhlane; Alseno K Mosai; Jessica Mhlongo; Aaliyah Khan; Karl Rumbold; Yannick B Nuapia
Journal:  AAS Open Res       Date:  2021-01-21

3.  Pretreatment of Japanese cedar by ionic liquid solutions in combination with acid and metal ion and its application to high solid loading.

Authors:  Kazuma Ogura; Kazuaki Ninomiya; Kenji Takahashi; Chiaki Ogino; Akihiko Kondo
Journal:  Biotechnol Biofuels       Date:  2014-08-20       Impact factor: 6.040

  3 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.