All-ceramic systems: laboratory and clinical performance.

Petra C Guess1, Stefan Schultheis, Estevam A Bonfante, Paulo G Coelho, Jonathan L Ferencz, Nelson R F A Silva.   

Abstract

Several all-ceramic systems have been developed in dentistry to meet the increased expectations of patients and dentists for highly aesthetic, biocompatible, and long-lasting restorations. However, early bulk fractures or chippings have led the research community to investigate the mechanical performance of the all-ceramic systems. This overview explores the current knowledge of monolithic and bilayer dental all-ceramic systems, addressing composition and processing mechanisms, laboratory and clinical performance, and possible future trends for all-ceramic materials.
Copyright © 2011 Elsevier Inc. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2011        PMID: 21473997     DOI: 10.1016/j.cden.2011.01.005

Source DB:  PubMed          Journal:  Dent Clin North Am        ISSN: 0011-8532


  34 in total

1.  Clinical evaluation of ceramic inlays and onlays fabricated with two systems: 12-year follow-up.

Authors:  Maria Jacinta Moraes Coelho Santos; Maria Cristina Freitas; Larissa Marinho Azevedo; Gildo Coelho Santos; Maria Fidela Navarro; Carlos Eduardo Francischone; Rafael Francisco Mondelli
Journal:  Clin Oral Investig       Date:  2015-12-12       Impact factor: 3.573

2.  Effect of thermocycling on flexural strength and weibull statistics of machinable glass-ceramic and composite resin.

Authors:  Chaimongkon Peampring; Sasiwimol Sanohkan
Journal:  J Indian Prosthodont Soc       Date:  2013-12-20

3.  Reliability of reduced-thickness and thinly veneered lithium disilicate crowns.

Authors:  N R F A Silva; E A Bonfante; L M Martins; G B Valverde; V P Thompson; J L Ferencz; P G Coelho
Journal:  J Dent Res       Date:  2011-12-28       Impact factor: 6.116

4.  Sub-ablative Er,Cr:YSGG laser irradiation under all-ceramic restorations: effects on demineralization and shear bond strength.

Authors:  Serdar Bağlar
Journal:  Lasers Med Sci       Date:  2017-09-17       Impact factor: 3.161

5.  Wear behavior of pressable lithium disilicate glass ceramic.

Authors:  Zhongxiao Peng; Muhammad Izzat Abdul Rahman; Yu Zhang; Ling Yin
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2015-05-15       Impact factor: 3.368

6.  Fracture Resistance and Fracture Behaviour of Monolithic Multi-Layered Translucent Zirconia Fixed Dental Prostheses with Different Placing Strategies of Connector: An in vitro Study.

Authors:  Nada Heidari; Rasha Amawi; Przemek Seweryniak; Fahad Bakitian; Per Vult von Steyern
Journal:  Clin Cosmet Investig Dent       Date:  2022-03-22

7.  Evaluation of Different Polishing Systems and Speeds for Dental Zirconia.

Authors:  Ramakiran Chavali; Chee Paul Lin; Nathaniel C Lawson
Journal:  J Prosthodont       Date:  2015-11-30       Impact factor: 2.752

8.  Three-unit CAD/CAM-generated lithium disilicate FDPs after a mean observation time of 46 months.

Authors:  Sven Reich; Lutz Endres; Claudia Weber; Klaus Wiedhahn; Peter Neumann; Oliver Schneider; Nicole Rafai; Stefan Wolfart
Journal:  Clin Oral Investig       Date:  2014-02-04       Impact factor: 3.573

9.  Evaluation of fracture resistance and mode of failure of premolars restored with nanohybrid composite, ORMOCER and ceramic inlays.

Authors:  Mohit K Gunwal; Pratima R Shenoi; Tanvee Paranjape; Sonal Dhote; Ravish Tongya; Magesh Kumar; Sanjay Rastogi
Journal:  J Oral Biol Craniofac Res       Date:  2017-09-01

10.  Advances in dental veneers: materials, applications, and techniques.

Authors:  Núbia Pavesi Pini; Flávio Henrique Baggio Aguiar; Débora Alves Nunes Leite Lima; José Roberto Lovadino; Raquel Sano Suga Terada; Renata Corrêa Pascotto
Journal:  Clin Cosmet Investig Dent       Date:  2012-02-10
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.