Literature DB >> 21323378

Uniform hollow Lu2O3:Ln (Ln = Eu3+, Tb3+) spheres: facile synthesis and luminescent properties.

Piaoping Yang1, Shili Gai, Yanchao Liu, Wenxin Wang, Chunxia Li, Jun Lin.   

Abstract

Uniform hollow Lu(2)O(3):Ln (Ln = Eu(3+), Tb(3+)) phosphors have been successfully prepared via a urea-assisted homogeneous precipitation method using carbon spheres as templates, followed by a subsequent calcination process. X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), Fourier transformed infrared (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), photoluminescence (PL) spectra, cathodoluminescence (CL) spectra, kinetic decays, quantum yields (QY), and UV-visible diffuse reflectance spectra were employed to characterize the samples. The results show that hollow Lu(2)O(3):Ln spheres can be indexed to cubic Gd(2)O(3) phase with high purity. The as-prepared hollow Lu(2)O(3):Ln phosphors are confirmed to be uniform in shape and size with diameter of about 300 nm and shell thickness of approximate 20 nm. The possible formation mechanism of evolution from the carbon spheres to the amorphous precursor and to the final hollow Lu(2)O(3):Ln microspheres has been proposed. Upon ultraviolet (UV) and low-voltage electron beams excitation, the hollow Lu(2)O(3):Ln (Ln = Eu(3+), Tb(3+)) spheres exhibit bright red (Eu(3+), (5)D(0)-(7)F(2)) and green (Tb(3+), (5)D(4)-(7)F(5)) luminescence, which may find potential applications in the fields of color display and biomedicine.

Entities:  

Mesh:

Substances:

Year:  2011        PMID: 21323378     DOI: 10.1021/ic101605k

Source DB:  PubMed          Journal:  Inorg Chem        ISSN: 0020-1669            Impact factor:   5.165


  1 in total

1.  Color-tunable properties of Eu3+- and Dy3+-codoped Y2O3 phosphor particles.

Authors:  Timur Sh Atabaev; Yoon-Hwae Hwang; Hyung-Kook Kim
Journal:  Nanoscale Res Lett       Date:  2012-10-08       Impact factor: 4.703