Literature DB >> 20944880

Bonding to densely sintered alumina- and glass infiltrated aluminum / zirconium-based ceramics.

Luiz Felipe Valandro1, André Mallmann, Alvaro Della Bona, Marco Antonio Bottino.   

Abstract

The objective of this study was to test two hypotheses: (1) silica coating affects the bond strength between ceramics and a resin cement; (2) bond strength is affected by the type of ceramic. Twelve blocks 5 x 6 x 8 mm of In-Ceram Zirconia (ZR) and twelve Procera AllCeram (PR) ceramics were made and duplicated in composite. Five blocks of each ceramic were treated as follows: (1) ZR + GB (laboratorial airborne particles abrasion with Al2O3 particles) + silane; (2) ZR + SC (chairside tribochemical silica coating system, Cojet); (3) PR + GB; (4) PR + SC. Two treated samples of ceramic were analyzed under SEM. The ceramic-composite blocks were cemented with Panavia F and stored in 37ºC distilled water for 7 days. They were then cut to produce bar specimens (n=30) with a bonding area of 0.6±0.1mm². Specimens were loaded to failure under tension in a universal testing machine (1 mm/min). Bond strength (sigma) values were statistically analyzed using ANOVA (Two-way) and Tukey (alpha = 0.05). Mean sigma (MPa) and standard deviation were as follows: 1) 15.1 ± 5.3; 2) 26.8 ± 7.4; 3) 12.7 ± 2.6; 4) 18.5 ± 4.7. Silica coated surfaces showed statistically higher sigma than the same substrate treated with GB only. In addition, ZR (with vitreous phase) showed higher ó than PR (without vitreous phase).

Entities:  

Year:  2005        PMID: 20944880     DOI: 10.1590/s1678-77572005000100010

Source DB:  PubMed          Journal:  J Appl Oral Sci        ISSN: 1678-7757            Impact factor:   2.698


  2 in total

Review 1.  Adhesion/cementation to zirconia and other non-silicate ceramics: where are we now?

Authors:  Jeffrey Y Thompson; Brian R Stoner; Jeffrey R Piascik; Robert Smith
Journal:  Dent Mater       Date:  2010-11-20       Impact factor: 5.304

2.  Bond strength of selected composite resin-cements to zirconium-oxide ceramic.

Authors:  Juan-Luis Román-Rodríguez; Antonio Fons-Font; Vicente Amigó-Borrás; María Granell-Ruiz; David Busquets-Mataix; Rubén-Agustín Panadero; Maria-Fernanda Solá-Ruiz
Journal:  Med Oral Patol Oral Cir Bucal       Date:  2013-01-01
  2 in total