Literature DB >> 20579856

Microscopic structural analysis of fractured silk fibers from Bombyx mori and Samia cynthia ricini using 13C CP/MAS NMR with a 1mm microcoil MAS NMR probehead.

Kazuo Yamauchi1, Shizuo Yamasaki, Rui Takahashi, Tetsuo Asakura.   

Abstract

Conformational changes have been studied in silk fibers from the domestic silkworm Bombyx mori and a wild silkworm Samia cynthia ricini as a result of fractured by stretching. About 300 samples consisting of only the fractured regions of [1-13C]Ala or [1-13C]Gly labeled silk fibers were collected and observed by 13C CP/MAS NMR spectra. The total amount of these fractured fibers is only about 1mg and therefore we used a home-built 1mm microcoil MAS NMR probehead. A very small increase in the fraction of random coil was noted for the alanine regions of both silk fibroins and for the glycine region of B. mori silk fibroin. However, there is no difference in the spectra before and after fractured for the glycine region of S. c. ricini silk fibroin. Thus, the influence of fracture occurs exclusively at the Ala region for S. c. ricini. The relationship between sequence, fracture and structure is discussed. 2010 Elsevier Inc. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2010        PMID: 20579856     DOI: 10.1016/j.ssnmr.2010.06.002

Source DB:  PubMed          Journal:  Solid State Nucl Magn Reson        ISSN: 0926-2040            Impact factor:   2.293


  2 in total

Review 1.  Structure of Silk I (Bombyx mori Silk Fibroin before Spinning) -Type II β-Turn, Not α-Helix.

Authors:  Tetsuo Asakura
Journal:  Molecules       Date:  2021-06-17       Impact factor: 4.411

2.  Glycerin-Induced Conformational Changes in Bombyx mori Silk Fibroin Film Monitored by (13)C CP/MAS NMR and ¹H DQMAS NMR.

Authors:  Tetsuo Asakura; Masanori Endo; Misaki Hirayama; Hiroki Arai; Akihiro Aoki; Yugo Tasei
Journal:  Int J Mol Sci       Date:  2016-09-09       Impact factor: 5.923

  2 in total