Abstract

BACKGROUND, AIM AND SCOPE: Weathering patinas in rocks are the result of interaction processes between rock surfaces and atmosphere, biosphere and soil. Therefore, their textural and mineral composition is strongly related to environmental and bioactivity conditions. Whereas the development of weathering patinas in atmospheric conditions is well documented (e.g. typical Mediterranean patina), only very few studies focus on their formation in a burial environment. Our study of patinas developed on the tumular structure of Reguers de Seró deals with the knowledge of burial patinas from a textural and mineralogical point of view. The aims of this study include: (1) the characterisation of the rock used in this megalithic monument as well as inferences regarding the origin of the raw material; (2) the evaluation of the patinas developed on the surface of the carved steles; and (3) the discussion of the environmental conditions (atmospheric or burial) that favoured the development of the patinas.
MATERIALS AND METHODS: Whole rock and related patinas (powdered samples and small single pieces) were carefully sampled in five of the seven Neolithic steles discovered during a municipal excavation. Some whole rock samples from the surrounding outcrops were also collected in order to correlate them with the stone forming the megalith. Samples were analysed macroscopically, using a glass binocular, and microscopically, by means of a polarising light microscope and a scanning electron microscope (SEM-EDAX). The mineralogical composition was determined by X-ray diffraction, and a colorimetric analysis was also carried out in all the sampled patinas.
RESULTS: The obtained results evidence a strong textural and mineralogical correlation between the whole rock of the megalith and the collected samples of the nearby outcrops; both are classified as calcarenite. A uniformly distributed beige-orange patina (35-100 microm thick) covering the surface of the steles modifies their aspect. A layer of calcite (micrite) with granular texture was detected in all the sampled patinas, being the main mineral compositions (approximately 60-90%). In contrast, a discontinuous external layer (25-50 microm thick) of botryoidally gypsum occurs on only a few patinas. SEM-EDAX analyses evidenced that Ca is related to several processes, including inorganic processes, as well as to minor bioactivity. DISCUSSION: The textural and mineralogical characteristics of the Reguers patinas differ from typical Mediterranean patina sequences, suggesting different environmental conditions for their formation. Several arguments supporting the formation of the Reguers patinas in a burial environment include: (1) patinas cover the entire surface of the steles, iconograhic motifs and fractures. The uniform colour, texture and composition of the patinas throughout the steles suggests their development after the construction of the megalithic tomb during a period in which the archaeological site was buried and sealed by the products of the Senill ravine; (2) the absence of heavy metals mainly contained in flying ashes and other depositions from atmospheric dust and pollutants in the micritic patina; (3) non-appearance of minerals directly formed by biological activity (i.e. oxalates and phosphates); (4) the absence of a well-defined textural sequence (typically of the Mediterranean area) already defined for patinas developed in an atmospheric environment; and (5) the discontinuous occurrence of an external gypsum layer (only present in a few samples) without the presence of the typical spherules related to atmospheric particulate matter. CONCLUSIONS AND RECOMMENDATIONS: The petrographic characteristics of the Neolithic steles of Reguers de Seró show that the raw material came from a nearby outcrop. The formation of beige-orange patinas is related to a burial environment attending their textural and mineralogical features. The protective role played by these patinas indicates that no previous treatment of such steles would be necessary on an eventual exhibition in atmospheric conditions. Further in-depth studies, similar to those that already exist for patinas developed in atmospheric conditions, are recommended in order to better define the petrographic characteristics and mechanisms on the formation of patinas in burial environments.

Entities:  

Mesh:

Substances:

Year:  2010        PMID: 20213307     DOI: 10.1007/s11356-010-0308-0

Source DB:  PubMed          Journal:  Environ Sci Pollut Res Int        ISSN: 0944-1344            Impact factor:   4.223


  6 in total

1.  Black layers on historical architecture.

Authors:  Lucia Toniolo; Carlotta M Zerbi; Roberto Bugini
Journal:  Environ Sci Pollut Res Int       Date:  2008-10-07       Impact factor: 4.223

2.  Renaissance patinas in Ubeda (Spain): mineralogic, petrographic and spectroscopic study.

Authors:  M J Campos-Suñol; A Domínguez-Vidal; M J Ayora-Cañada; M J De la Torre-López
Journal:  Anal Bioanal Chem       Date:  2008-04-30       Impact factor: 4.142

3.  The orange-brown patina of Salisbury Cathedral (West Porch) surfaces: evidence of its man-made origin.

Authors:  Jesus Martín-Gil; Francisco Javier Martín-Gil; Maria del Carmen Ramos-Sánchez; Pablo Martín-Ramos
Journal:  Environ Sci Pollut Res Int       Date:  2005-09       Impact factor: 4.223

4.  Weathering patinas on the medieval (S. XIV) stained glass windows of the Pedralbes Monastery (Barcelona, Spain).

Authors:  Meritxell Aulinas; Maite Garcia-Valles; Domingo Gimeno; Jose Luis Fernandez-Turiel; Flavia Ruggieri; Montserrat Pugès
Journal:  Environ Sci Pollut Res Int       Date:  2008-12-23       Impact factor: 4.223

5.  Analytical investigation of calcium oxalate films on marble monuments.

Authors:  L Rampazzi; A Andreotti; I Bonaduce; M P Colombini; C Colombo; L Toniolo
Journal:  Talanta       Date:  2004-07-08       Impact factor: 6.057

6.  Multi-disciplinary characterisation of a sandstone surface crust.

Authors:  Cnudde Veerle; Silversmit Geert; Boone Matthieu; Dewanckele Jan; De Samber Björn; Schoonjans Tom; Van Loo Denis; De Witte Yoni; Elburg Marlina; Vincze Laszlo; Van Hoorebeke Luc; Jacobs Patric
Journal:  Sci Total Environ       Date:  2009-07-25       Impact factor: 7.963

  6 in total
  1 in total

1.  Microscopic, chemical, and molecular-biological investigation of the decayed medieval stained window glasses of two Catalonian churches.

Authors:  Guadalupe Piñar; Maite Garcia-Valles; Domingo Gimeno-Torrente; Jose Luis Fernandez-Turiel; Jörg Ettenauer; Katja Sterflinger
Journal:  Int Biodeterior Biodegradation       Date:  2013-10       Impact factor: 4.320

  1 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.