Literature DB >> 19939446

Corrosion of, and cellular responses to Mg-Zn-Ca bulk metallic glasses.

Xuenan Gu1, Yufeng Zheng, Shengping Zhong, Tingfei Xi, Junqiang Wang, Weihua Wang.   

Abstract

Mg-Zn-Ca bulk metallic glass with different compositions (Mg66Zn30Ca4 and Mg70Zn25Ca5) have been prepared for this study and their feasibility as biodegradable metallic materials have been evaluated by the microstructural, surface analysis, mechanical testing, corrosion and cytotoxicity tests. It was found that the Mg66Zn30Ca4 sample presents a more uniform corrosion morphology than as-rolled pure Mg and Mg70Zn25Ca5 samples, with much smaller micro-scale uniformly distributed pores beneath the corrosion product layer. The corrosion products were identified to be Mg(OH)(2) and Zn(OH)(2), and a uniform corrosion mechanism is proposed. Both indirect cytotoxicity and direct cell culture experiments were carried out using L929 and MG63 cell lines. The results show higher cell viabilities for Mg-Zn-Ca extracts than that for as-rolled pure Mg. In addition, L929 and MG63 cells were found to adhere and proliferate on the surface of Mg66Zn30Ca4 sample. (c) 2009 Elsevier Ltd. All rights reserved.

Entities:  

Mesh:

Substances:

Year:  2009        PMID: 19939446     DOI: 10.1016/j.biomaterials.2009.11.015

Source DB:  PubMed          Journal:  Biomaterials        ISSN: 0142-9612            Impact factor:   12.479


  27 in total

1.  Endothelial responses of magnesium and other alloying elements in magnesium-based stent materials.

Authors:  Nan Zhao; Donghui Zhu
Journal:  Metallomics       Date:  2014-11-03       Impact factor: 4.526

2.  In vitro biocompatibility assessment of Ti40Cu38Zr10Pd12 bulk metallic glass.

Authors:  A Blanquer; E Pellicer; A Hynowska; L Barrios; E Ibáñez; M D Baró; J Sort; C Nogués
Journal:  J Mater Sci Mater Med       Date:  2014-01       Impact factor: 3.896

3.  Nd-induced honeycomb structure of intermetallic phase enhances the corrosion resistance of Mg alloys for bone implants.

Authors:  Cijun Shuai; Youwen Yang; Shuping Peng; Chengde Gao; Pei Feng; Jian Chen; Yong Liu; Xin Lin; Sheng Yang; Fulai Yuan
Journal:  J Mater Sci Mater Med       Date:  2017-07-20       Impact factor: 3.896

4.  Investigation of the antimicrobial activity and biocompatibility of magnesium alloy coated with HA and antimicrobial peptide.

Authors:  Jinhuan Tian; Si Shen; Changren Zhou; Xiangli Dang; Yanpeng Jiao; Lihua Li; Shan Ding; Hong Li
Journal:  J Mater Sci Mater Med       Date:  2015-01-29       Impact factor: 3.896

Review 5.  Zinc-based alloys for degradable vascular stent applications.

Authors:  Ehsan Mostaed; Malgorzata Sikora-Jasinska; Jaroslaw W Drelich; Maurizio Vedani
Journal:  Acta Biomater       Date:  2018-03-10       Impact factor: 8.947

6.  Buffer-regulated biocorrosion of pure magnesium.

Authors:  Nicholas T Kirkland; Jay Waterman; Nick Birbilis; George Dias; Tim B F Woodfield; Richard M Hartshorn; Mark P Staiger
Journal:  J Mater Sci Mater Med       Date:  2011-12-22       Impact factor: 3.896

7.  Cellular reactions to biodegradable magnesium alloys on human growth plate chondrocytes and osteoblasts.

Authors:  Karin Pichler; Tanja Kraus; Elisabeth Martinelli; Patrick Sadoghi; Giuseppe Musumeci; Peter J Uggowitzer; Annelie M Weinberg
Journal:  Int Orthop       Date:  2013-11-21       Impact factor: 3.075

8.  Implant-derived magnesium induces local neuronal production of CGRP to improve bone-fracture healing in rats.

Authors:  Yifeng Zhang; Jiankun Xu; Ye Chun Ruan; Mei Kuen Yu; Micheal O'Laughlin; Helen Wise; Di Chen; Li Tian; Dufang Shi; Jiali Wang; Sihui Chen; Jian Q Feng; Dick Ho Kiu Chow; Xinhui Xie; Lizhen Zheng; Le Huang; Shuo Huang; Kwoksui Leung; Na Lu; Lan Zhao; Huafang Li; Dewei Zhao; Xia Guo; Kaiming Chan; Frank Witte; Hsiao Chang Chan; Yufeng Zheng; Ling Qin
Journal:  Nat Med       Date:  2016-08-29       Impact factor: 53.440

9.  Cytocompatibility of magnesium and AZ31 alloy with three types of cell lines using a direct in vitro method.

Authors:  Akira Mochizuki; Chie Yahata; Hung Takai
Journal:  J Mater Sci Mater Med       Date:  2016-08-27       Impact factor: 3.896

10.  Structural characteristics and corrosion behavior of biodegradable Mg-Zn, Mg-Zn-Gd alloys.

Authors:  J Kubásek; D Vojtěch
Journal:  J Mater Sci Mater Med       Date:  2013-03-26       Impact factor: 3.896

View more