PURPOSE: The aim of this clinical study was to observe the service duration of porcelain laminate veneers (PLVs) and to estimate the influence of the categorical covariates such as location, tooth vitality, preparation depth, incisal, gingival and proximal finishing lines, and peripheral tissue type on the survival rates of event-free and overall service duration.
MATERIALS AND METHODS: A total of forty patients (26 women, 14 men; age range: 16 to 50) who had received 200 PLVs were evaluated in this study. Median follow-up time was 67.25 weeks with a range of 12 to 72 weeks. Fifteen of the restored teeth were nonvital, while the remaining 185 were vital. Categorical covariates related to the restoration design (localization, vitality, preparation depth, incisal, proximal, and gingival finishings, and surrounding tissue type) were recorded in order to estimate their influence on the survival rates. Survival rates of the event-free and overall service duration were calculated with the Kaplan-Meier analysis and Mantel log rank test.
RESULTS: Twelve failures were observed. The most frequent failure type (11 units) was debonding of the restoration from the abutment tooth. Nine of them were rebonded and the remaining 2 were remade with a different preparation design. The last failure was observed as a coronal fracture at the cervical level. The overall survival rates were 99.5%, 99%, 97.5%, 94.9%, 94.4% and 93.8% at weeks 8, 9, 11, 15, 16, and 34, respectively, with a mean estimate of 68.45 weeks.
CONCLUSION: PLVs exhibited good clinical results with their conservative specifications and high survival rates. The preparation and design specifications affect the service duration of PLVs.

Entities:  

Mesh:

Substances:

Year:  2009        PMID: 19841768

Source DB:  PubMed          Journal:  J Adhes Dent        ISSN: 1461-5185            Impact factor:   2.359


  7 in total

1.  Sub-ablative Er,Cr:YSGG laser irradiation under all-ceramic restorations: effects on demineralization and shear bond strength.

Authors:  Serdar Bağlar
Journal:  Lasers Med Sci       Date:  2017-09-17       Impact factor: 3.161

2.  Clinical evaluation on porcelain laminate veneers bonded with light-cured composite: results up to 7 years.

Authors:  Camillo D'Arcangelo; Francesco De Angelis; Mirco Vadini; Maurizio D'Amario
Journal:  Clin Oral Investig       Date:  2011-07-20       Impact factor: 3.573

3.  The Effect of Polymerization and Preparation Techniques on the Microleakage of Composite Laminate Veneers.

Authors:  Neslihan Celik; Merve Iscan Yapar; Numan Taşpınar; Nilgun Seven
Journal:  Contemp Clin Dent       Date:  2017 Jul-Sep

4.  Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading.

Authors:  Leyla Sadighpour; Farideh Geramipanah; Vanya Rasaei; Mohammad J Kharazi Fard
Journal:  Int J Dent       Date:  2018-04-17

5.  Fracture Resistance of Upper Central Incisors with Different Endodontic Accesses Restored with Lithium Disilicate Partial Laminate Veneers.

Authors:  Hamit Serdar Cotert; Ilgin Akcay; Irem Cotert; Ece Altinova Hepdurgun
Journal:  Clin Cosmet Investig Dent       Date:  2021-12-29

6.  Survival Rates for Porcelain Laminate Veneers: A Systematic Review.

Authors:  Yousra H AlJazairy
Journal:  Eur J Dent       Date:  2020-10-01

7.  Esthetic rehabilitation of anterior teeth with different thicknesses of porcelain laminate veneers: An 8-year follow-up clinical evaluation.

Authors:  Tassiana Cançado Melo Sá; Monize Ferreira Figueiredo de Carvalho; Julio Celso M de Sá; Claudia Silami Magalhães; Allyson Nogueira Moreira; Monica Yamauti
Journal:  Eur J Dent       Date:  2018 Oct-Dec
  7 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.