Lauro Egídio Bragaglia1, Luiz Henrique Maykot Prates, Maria Cristina Marino Calvo.
Abstract
The aim of this study was to compare the bond strength between acrylic denture base and teeth subjected to 6 surface treatments. Ninety-six specimens were made with poly(methylmethacrylate) teeth bonded to a microwave-polymerized acrylic denture base material. The specimens were distributed into 6 groups (n=16) according to surface treatments: CT - no treatment (control); MN - methylmethacrylate monomer etching; AO - 50-microm-particle aluminum oxide air abrasion; BR - glaze removal with a round bur; ST - surface grinding with an aluminum oxide abrasive stone; group CV - cavity preparation (diatorics). The control and surface-treated groups were subjected to a compressive load at 45 masculine angle to the long axis of the teeth. Data were analyzed by one-way ANOVA, followed by Scheffé's test (p<0.05). Bond strength means and (SD) in kgf for groups were: CT: 18.19 (7.14), MN: 18.34 (5.28), AO: 23.82 (5.40), BR: 23.30 (4.79), ST: 25.39 (7.80) and CV: 17.48 (7.17). There was statistically significant difference (p=0.037997) only between ST and CV. In conclusion, ridge lap surface grinding with an aluminum oxide abrasive stone provided the highest bond strength, though it differed significantly only when compared to diatorics. The other surface treatments provided similar bond between the acrylic denture base and teeth.Entities:
Mesh:
Substances:
Year: 2009 PMID: 19738950 DOI: 10.1590/s0103-64402009000200012
Source DB: PubMed Journal: Braz Dent J ISSN: 0103-6440