| Literature DB >> 1941662 |
H Matsumura1, M Kawahara, T Tanaka, M Atsuta.
Abstract
Bond strengths of a laboratory developed light-cured composite resin to dental casting alloys were evaluated with a new adhesive opaque resin. The metal specimens were type III gold, nickel-chromium, and cobalt-chromium alloys, while the surface treatments for bonding were heating, Sn plating, and ion coating. The cast metal specimens were "particle blasted" with aluminum oxide and were surface treated. Adhesive 4-META/MMA-TBB opaque resin was applied and a light-cured composite resin was placed over the opaque layer. The prepared specimens were thermocycled in water and shear bond strengths were recorded. The light-cured composite resin was bonded strongly to heated or Sn-plated type III alloy with 4-META/MMA-TBB opaque resin. Copper ion coating in a sputter coater was effective for all three alloys, with only slightly diminished bond strengths. These methods were satisfactory for making composite resin veneered prostheses.Entities:
Mesh:
Substances:
Year: 1991 PMID: 1941662 DOI: 10.1016/0022-3913(91)90343-u
Source DB: PubMed Journal: J Prosthet Dent ISSN: 0022-3913 Impact factor: 3.426