T H Mahato1, G K Prasad, Beer Singh, J Acharya, A R Srivastava, R Vijayaraghavan.
Abstract
Nanocrystalline zinc oxide materials were prepared by sol-gel method and were characterized by X-ray diffraction, scanning electron microscopy, thermogravimetry, nitrogen adsorption and infrared spectroscopy techniques. The data confirmed the formation of zinc oxide materials of zincite phase with an average crystallite size of approximately 55 nm. Obtained material was tested as destructive adsorbent for the decontamination of sarin and the reaction was followed by GC-NPD and GC-MS techniques. The reaction products were characterized by GC-MS and the data explored the role of hydrolysis reaction in the detoxification of sarin. Sarin was hydrolyzed to form surface bound non-toxic phosphonate on the surface of nano-zinc oxide. The data also revealed the values of rate constant and half-life to be 4.12h(-1) and 0.16 h in the initial stages of the reaction and 0.361 h(-1) and 1.9h at the final stages of the reaction for the decontamination reaction on nanocrystalline ZnO.Entities:
Mesh:
Substances:
Year: 2008 PMID: 19121895 DOI: 10.1016/j.jhazmat.2008.10.126
Source DB: PubMed Journal: J Hazard Mater ISSN: 0304-3894 Impact factor: 10.588