Literature DB >> 18717176

Evaluation of flowable resin composite surfaces eroded by acidic and alcoholic drinks.

Linlin Han1, Akira Okamoto, Masayoshi Fukushima, Takashi Okiji.   

Abstract

The purpose of this study was to evaluate the morphological changes of the surfaces of flowable resins eroded by orange juice and alcohol drinks. The tested products were Beautifil Flow BF02 and BF10, Clearfil Majesty LV, Filtek Supreme XT Flowable Restorative, Unifil LoFlo Plus and Filtek Supreme. Filler percentages of flowable resins were calculated after the latter were incinerated at 750 degrees C. Specimens were shaped into a disk form with a diameter of 10 mm and a thickness of 1 mm. Morphological changes were evaluated for the following types of flowable resin surfaces: polished surface, surfaces eroded by 100% orange juice, wine and whisky. Filler percentages of the tested flowable resins ranged between 42 and 78%. Surface degradation was observed for the specimens immersed in acidic and alcoholic drinks, and it was thought that the lower the filler percentage, the greater was the surface degradation. Decomposition of the matrix resin and fallout of the fillers were observed in flowable resins that eroded with acidic and alcoholic drinks.

Entities:  

Mesh:

Substances:

Year:  2008        PMID: 18717176     DOI: 10.4012/dmj.27.455

Source DB:  PubMed          Journal:  Dent Mater J        ISSN: 0287-4547            Impact factor:   2.102


  14 in total

Review 1.  Flowable Resin Composites: A Systematic Review and Clinical Considerations.

Authors:  Kusai Baroudi; Jean C Rodrigues
Journal:  J Clin Diagn Res       Date:  2015-06-01

2.  Randomized controlled clinical trial of a highly filled flowable composite in non-carious cervical lesions: 3-year results.

Authors:  Haiying Zhang; Luxuan Wang; Lin Hua; Rui Guan; Benxiang Hou
Journal:  Clin Oral Investig       Date:  2021-04-02       Impact factor: 3.573

3.  Influence of cleaning methods after 3D printing on two-body wear and fracture load of resin-based temporary crown and bridge material.

Authors:  Johannes Mayer; Bogna Stawarczyk; Konstantin Vogt; Reinhard Hickel; Daniel Edelhoff; Marcel Reymus
Journal:  Clin Oral Investig       Date:  2021-04-03       Impact factor: 3.573

4.  Determinants of enamel decalcification during simulated orthodontic treatment.

Authors:  Elizabeth Hess; Phillip M Campbell; Allen L Honeyman; Peter H Buschang
Journal:  Angle Orthod       Date:  2011-05-05       Impact factor: 2.079

5.  Does the amount of filler content in sealants used to prevent decalcification on smooth enamel surfaces really matter?

Authors:  Lauren Van Bebber; Phillip M Campbell; Allen L Honeyman; Robert Spears; Peter H Buschang
Journal:  Angle Orthod       Date:  2011-01       Impact factor: 2.079

6.  Surface roughness of flowable resin composites eroded by acidic and alcoholic drinks.

Authors:  Claudio Poggio; Alberto Dagna; Marco Chiesa; Marco Colombo; Andrea Scribante
Journal:  J Conserv Dent       Date:  2012-04

7.  Erosive potential of cola and orange fruit juice on tooth colored restorative materials.

Authors:  K Rajavardhan; Ajs Sankar; Mgm Kumar; Kr Kumar; K Pranitha; Kk Kishore
Journal:  Ann Med Health Sci Res       Date:  2014-09

8.  Flexural Properties and Elastic Modulus of Different Esthetic Restorative Materials: Evaluation after Exposure to Acidic Drink.

Authors:  Andrea Scribante; Marco Bollardi; Marco Chiesa; Claudio Poggio; Marco Colombo
Journal:  Biomed Res Int       Date:  2019-02-04       Impact factor: 3.411

9.  The effect of different beverages on surface hardness of nanohybrid resin composite and giomer.

Authors:  Saijai Tanthanuch; Boonlert Kukiattrakoon; Chantima Siriporananon; Nawanda Ornprasert; Wathu Mettasitthikorn; Salinla Likhitpreeda; Sulawan Waewsanga
Journal:  J Conserv Dent       Date:  2014-05

10.  Change in surface roughness of esthetic restorative materials after exposure to different immersion regimes in a cola drink.

Authors:  Navroop Kaur Bajwa; Anuradha Pathak
Journal:  ISRN Dent       Date:  2014-03-23
View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.