Literature DB >> 18309620

Discoloration and dissolution of titanium and titanium alloys with immersion in peroxide- or fluoride-containing solutions.

Tatsumi Noguchi1, Shinji Takemoto, Masayuki Hattori, Masao Yoshinari, Eiji Kawada, Yutaka Oda.   

Abstract

This study compared differences in discoloration and dissolution in several titanium alloys with immersion in peroxide- or fluoride-containing solution. Commercially pure titanium (CP-Ti) and six titanium-based alloys were used: Ti-0.15Pd, Ti-6Al-4V, Ti-7Nb-6Al, Ti-55Ni, Ti-10Cu, and Ti-20Cr. Two test solutions were prepared for immersion of polished titanium and titanium alloys: one consisting of 0.2% NaF + 0.9% NaCl (pH 3.8 with lactic acid) and the other of 0.1 mol/l H2O2 + 0.9% NaCl (pH 5.5). Following immersion, color changes were determined with a color meter and released elements were measured using ICP-OES. Discoloration and dissolution rates differed between the two solutions. In the hydrogen peroxide-containing solution, color difference was higher in Ti-55Ni and Ti-6Al-4V than in any of the other alloys, and that Ti-55Ni showed the highest degree of dissolution. In the acidulated fluoride-containing solution, CP-Ti, Ti-0.15Pd, Ti-6Al-4V, Ti-7Nb-6Al, and Ti-10Cu alloys showed remarkable discoloration and dissolution with immersion. On the contrary, Ti-20Cr alloy showed very little discoloration and dissolution in either solution.

Entities:  

Mesh:

Substances:

Year:  2008        PMID: 18309620     DOI: 10.4012/dmj.27.117

Source DB:  PubMed          Journal:  Dent Mater J        ISSN: 0287-4547            Impact factor:   2.102


  8 in total

1.  Influence of noble metals alloying additions on the corrosion behaviour of titanium in a fluoride-containing environment.

Authors:  F Rosalbino; S Delsante; G Borzone; G Scavino
Journal:  J Mater Sci Mater Med       Date:  2012-03-02       Impact factor: 3.896

2.  Spontaneous Fractures of a Modern Modular Uncemented Femoral Stem.

Authors:  Chelsea N Koch; Laura Serrano Mateo; Stephen Kayiaros; Kevin A Cassidy; Seth A Jerabek; Alejandro Gonzalez Della Valle
Journal:  HSS J       Date:  2016-06-21

3.  Brushing-induced surface roughness of two nickel based alloys and a titanium based alloy: a comparative study - in vitro study.

Authors:  B L Guruprasanna Acharya; Ramesh Nadiger; Bharathraj Shetty; G Gururaj; K Naveen Kumar; D D Darshan
Journal:  J Int Oral Health       Date:  2014-06-26

4.  Fretting Corrosion Behavior of Experimental Ti-20Cr Compared to Titanium.

Authors:  Tomofumi Sawada; Christine Schille; Atif Almadani; Jürgen Geis-Gerstorfer
Journal:  Materials (Basel)       Date:  2017-02-17       Impact factor: 3.623

5.  Alterations to Titanium Surface Depending on the Fluorides and Abrasives in Toothpaste.

Authors:  Takahiro Shuto; Yuichi Mine; Seicho Makihira; Hiroki Nikawa; Takanori Wachi; Kazutoshi Kakimoto
Journal:  Materials (Basel)       Date:  2021-12-22       Impact factor: 3.623

6.  Microstructural Modification of TiAl6V4 Alloy to Avoid Detrimental Effects Due to Selective In Vivo Crevice Corrosion.

Authors:  Maria Herbster; Karsten Harnisch; Paulina Kriegel; Andreas Heyn; Manja Krüger; Christoph H Lohmann; Jessica Bertrand; Thorsten Halle
Journal:  Materials (Basel)       Date:  2022-08-19       Impact factor: 3.748

7.  Effect of Topical Fluoride on Surface of Cast Titanium and Nickel-Chromium: An In Vitro Study.

Authors:  Gayatri Sheena Suvarna; Ramesh Khandurao Nadiger; Omkar Shetty
Journal:  J Dent (Tehran)       Date:  2015-06

8.  Mechanistic insight on the combined effect of albumin and hydrogen peroxide on surface oxide composition and extent of metal release from Ti6Al4V.

Authors:  Yolanda S Hedberg; Monika Žnidaršič; Gunilla Herting; Ingrid Milošev; Inger Odnevall Wallinder
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2018-08-13       Impact factor: 3.368

  8 in total