A comparison of the abrasiveness of six ceramic surfaces and gold.

R Jacobi1, H T Shillingburg, M G Duncanson.   

Abstract

A type III gold alloy and six different ceramic surfaces were secured in an abrasion machine opposing extracted teeth to determine their relative abrasiveness and resistance to wear. The rankings of restorative materials from least abrasive to most abrasive were: gold alloy, polished; cast ceramic, polished; porcelain, polished; cast ceramic, polished and shaded; porcelain, polished and glazed; cast ceramic, cerammed skin shaded; and cast ceramic, cerammed skin unshaded. The ranking of materials from most wear-resistant to least wear-resistant was: gold alloy, cast ceramic cerammed, cast ceramic cerammed and shaded, porcelain polished, porcelain glazed, cast ceramic polished and shaded, and cast ceramic polished.

Entities:  

Mesh:

Substances:

Year:  1991        PMID: 1800724     DOI: 10.1016/0022-3913(91)90254-t

Source DB:  PubMed          Journal:  J Prosthet Dent        ISSN: 0022-3913            Impact factor:   3.426


  9 in total

1.  Wear behavior and abrasiveness of monolithic CAD/CAM ceramics after simulated mastication.

Authors:  Ahmed Mahmoud Fouda; Osama Atta; Amr Shebl Kassem; Mohamed Desoky; Christoph Bourauel
Journal:  Clin Oral Investig       Date:  2022-07-11       Impact factor: 3.606

2.  Effect of veneering material on the deformation suffered by implant-supported fixed prosthesis framework.

Authors:  Antônio Francisco Grando; Carlos Eduardo Edwards Rezende; Edson Antônio Capello Sousa; José Henrique Rubo
Journal:  J Appl Oral Sci       Date:  2014-06       Impact factor: 2.698

3.  Esthetic Prosthetic Restorations: Reliability and Effects on Antagonist Dentition.

Authors:  Elie E Daou
Journal:  Open Dent J       Date:  2015-12-31

Review 4.  Advancements in all-ceramics for dental restorations and their effect on the wear of opposing dentition.

Authors:  Haroon Rashid; Zeeshan Sheikh; Syed Misbahuddin; Murtaza Raza Kazmi; Sameer Qureshi; Muhammad Zuhaib Uddin
Journal:  Eur J Dent       Date:  2016 Oct-Dec

5.  Effect of Three Commonly Consumed Beverages on Surface Roughness of Polished and Glazed Zirconia-Reinforced Lithium Silicate Glass Ceramics.

Authors:  Farnaz Firouz; Fariborz Vafaee; Zahra Khamverdi; Sara Khazaei; Somayeh Ghorbani Gholiabad; Mahsa Mohajeri
Journal:  Front Dent       Date:  2019-08-30

Review 6.  Wear Behavior of Different Generations of Zirconia: Present Literature.

Authors:  Kuljirarnat Jitwirachot; Pimduen Rungsiyakull; Julie A Holloway; Wissanee Jia-Mahasap
Journal:  Int J Dent       Date:  2022-03-07

Review 7.  Tooth wear against ceramic crowns in posterior region: a systematic literature review.

Authors:  Rim Hmaidouch; Paul Weigl
Journal:  Int J Oral Sci       Date:  2013-10-18       Impact factor: 6.344

8.  Effect of two different finishing systems on surface roughness of feldspathic and fluorapatite porcelains in ceramo-metal restorations: Comparative in vitro study.

Authors:  Cherry Anmol; Sumeet Soni
Journal:  J Int Soc Prev Community Dent       Date:  2014-01

9.  Comparison of the effect of monolithic and layered zirconia on natural teeth wear: An in vitro study.

Authors:  Yamini Gundugollu; Ravi Shankar Yalavarthy; M Hari Krishna; Srinivas Kalluri; Shameen Kumar Pydi; Satyendra Kumar Tedlapu
Journal:  J Indian Prosthodont Soc       Date:  2018 Oct-Dec
  9 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.