Making ceramics "ductile".

B R Lawn, N P Padture, H Cait, F Guiberteau.   

Abstract

Distributed irreversible deformation in otherwise brittle ceramics (specifically, in silicon carbide and micaceous glass-ceramic) has been observed in Hertzian contacts. The deformation takes the form of an expanding microcrack damage zone below the contact circle, in place of the usual single propagating macrocrack (the Hertzian "cone fracture") outside. An important manifestation of this deformation is an effective "ductility" in the indentation stress-strain response. Control of the associated brittle-ductile transition is readily effected by appropriate design of weak interfaces, large and elongate grains, and high internal stresses in the ceramic microstructure.

Entities:  

Year:  1994        PMID: 17831623     DOI: 10.1126/science.263.5150.1114

Source DB:  PubMed          Journal:  Science        ISSN: 0036-8075            Impact factor:   47.728


  11 in total

1.  Design maps for failure of all-ceramic layer structures in concentrated cyclic loading.

Authors:  Sanjit Bhowmick; Juan José Meléndez-Martínez; Yu Zhang; Brian R Lawn
Journal:  Acta Mater       Date:  2007-04-01       Impact factor: 8.203

2.  Inverse correlations between wear and mechanical properties in biphasic dental materials with ceramic constituents.

Authors:  Oscar Borrero-Lopez; Fernando Guiberteau; Yu Zhang; Brian R Lawn
Journal:  J Mech Behav Biomed Mater       Date:  2020-03-12

3.  3D-WOVEN FIBER-REINFORCED COMPOSITE FOR CAD/CAM DENTAL APPLICATION.

Authors:  Richard Petersen; Perng-Ru Liu
Journal:  Sampe J       Date:  2016-05       Impact factor: 0.182

4.  Influence of preparation design and ceramic thicknesses on fracture resistance and failure modes of premolar partial coverage restorations.

Authors:  Petra C Guess; Stefan Schultheis; Martin Wolkewitz; Yu Zhang; Joerg R Strub
Journal:  J Prosthet Dent       Date:  2013-10       Impact factor: 3.426

5.  Competition of fracture mechanisms in monolithic dental ceramics: flat model systems.

Authors:  Yu Zhang; Jae-Won Kim; Sanjit Bhowmick; Van P Thompson; E Dianne Rekow
Journal:  J Biomed Mater Res B Appl Biomater       Date:  2009-02       Impact factor: 3.368

6.  Hardness properties and microscopic investigation of crack- crystal interaction in SiO(2)-MgO-Al(2)O(3)-K(2)O-B(2)O(3)-F glass ceramic system.

Authors:  Shibayan Roy; Bikramjit Basu
Journal:  J Mater Sci Mater Med       Date:  2010-01       Impact factor: 3.896

7.  Micromechanics of Machining and Wear in Hard and Brittle Materials.

Authors:  Brian R Lawn; Oscar Borrero-Lopez; Han Huang; Yu Zhang
Journal:  J Am Ceram Soc       Date:  2020-09-27       Impact factor: 3.784

Review 8.  Fatigue of dental ceramics.

Authors:  Yu Zhang; Irena Sailer; Brian R Lawn
Journal:  J Dent       Date:  2013-10-14       Impact factor: 4.379

9.  Origin of flaw-tolerance in nacre.

Authors:  Zaiwang Huang; Xiaodong Li
Journal:  Sci Rep       Date:  2013       Impact factor: 4.379

10.  Unique mechanical properties of nanostructured transparent MgAl2O4 ceramics.

Authors:  Jie Zhang; Tiecheng Lu; Xianghui Chang; Nian Wei; Jianqi Qi
Journal:  Nanoscale Res Lett       Date:  2013-06-01       Impact factor: 4.703

View more

北京卡尤迪生物科技股份有限公司 © 2022-2023.