Influence of the mechanical properties of composites for indirect dental restorations on pattern failure.

Michel Espinosa Klymus1, Rosemary Sadami Arai Shinkai, Eduardo Gonçalves Mota, Hugo Mitsuo Silva Oshima, Ana Maria Spohr, Luiz Henrique Burnett.   

Abstract

This study evaluated the fracture pattern of four composites for indirect dental restoration relating to three-point flexural strength, compressive strength and modulus of elasticity (Solidex, Artglass, belleGlass, and Targis). Ten specimens of each composite were tested in a universal testing machine at 0.5 mm/min crosshead speed for flexural strength and 1mm/min for compressive strength. Fracture pattern was classified as complete or partial fracture. Modulus of elasticity was calculated from flexural strength data. Composites polymerized under high temperatures (belleGlass and Targis) had higher flexural strength and elastic modulus values than composites polymerized by light (Artglass and Solidex). However, they failed earlier under compression because they were more rigid and showed partial fracture in the material bulk.

Entities:  

Mesh:

Substances:

Year:  2007        PMID: 17637528

Source DB:  PubMed          Journal:  Stomatologija        ISSN: 1392-8589


  3 in total

1.  Biological and Mechanical Evaluation of Novel Prototype Dental Composites.

Authors:  H L Van der Laan; S L Zajdowicz; K Kuroda; B J Bielajew; T A Davidson; J Gardinier; D H Kohn; S Chahal; S Chang; J Liu; J Gerszberg; T F Scott; B H Clarkson
Journal:  J Dent Res       Date:  2018-09-06       Impact factor: 6.116

2.  Indirect resin composites.

Authors:  Suresh Nandini
Journal:  J Conserv Dent       Date:  2010-10

3.  Three-year clinical performance of two indirect composite inlays compared to direct composite restorations.

Authors:  Nurcan Ozakar-Ilday; Yahya-Orcun Zorba; Mehmet Yildiz; Vildan Erdem; Nilgun Seven; Sezer Demirbuga
Journal:  Med Oral Patol Oral Cir Bucal       Date:  2013-05-01
  3 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.