| Literature DB >> 17570384 |
Sung-Hak Yi1, Seung-Kyu Choi, Jae-Min Jang, Jung-A Kim, Woo-Gwang Jung.
Abstract
Aligned ZnO nanorod arrays were synthesized using a chemical bath deposition method at normal atmospheric pressure without any metal catalyst. A simple two-step process was developed for growing ZnO nanorods on a PET substrate at 90-95 degrees C. The ZnO seed precursor was prepared by a sol-gel reaction. ZnO nanorod arrays were fabricated on ZnO-seed-coated substrate. The ZnO seeds were indispensable for the aligned growth of ZnO nanorods. The ZnO nanorods had a length of 400-500 nm and a diameter of 25-50 nm. HR-TEM and XRD analysis confirmed that the ZnO nanorod is a single crystal with a wurtzite structure and its growth direction is [0001] (the c-axis). Photoluminescence measurements of ZnO nanorods revealed an intense ultraviolet peak at 378.3 nm (3.27 eV) at room temperature.Entities:
Year: 2007 PMID: 17570384 DOI: 10.1016/j.jcis.2007.05.006
Source DB: PubMed Journal: J Colloid Interface Sci ISSN: 0021-9797 Impact factor: 8.128