Literature DB >> 17546416

Two different types of age-hardening behaviors in commercial dental gold alloys.

Kunihiro Hisatsune1, Takanobu Shiraishi, Yasuko Takuma, Yasuhiro Tanaka, Rhodora H Luciano.   

Abstract

Age-hardening behavior during continuous heating in commercial dental casting gold alloys was investigated by means of electrical resistivity measurements, hardness tests and X-ray diffraction. Two distinguishable behaviors were detected. It is considered that the difference was attributed to the amount of platinum, and the atomic ratio of gold and copper in each alloy. The phase transformations during continuous heating progressed into two steps (stages I and II). Increase of the platinum addition in gold-based alloys retards the rate of the reaction and decreases remarkably the amount of stage I.

Entities:  

Mesh:

Substances:

Year:  2007        PMID: 17546416     DOI: 10.1007/s10856-007-2304-6

Source DB:  PubMed          Journal:  J Mater Sci Mater Med        ISSN: 0957-4530            Impact factor:   3.896


  6 in total

1.  Phase transformation mechanisms in (AuCu)1-xPdx pseudobinary alloys by direct aging method.

Authors:  R I Hernandez; K Udoh; Y Tanaka; Y Takuma; H Winn; K Hisatsune
Journal:  Dent Mater J       Date:  1999-09       Impact factor: 2.102

2.  Ageing reactions in a high carat gold alloy for dental porcelain bonding.

Authors:  K Hisatsune; Y Tanaka; K Udoh; K Yasuda
Journal:  J Mater Sci Mater Med       Date:  1997-05       Impact factor: 3.896

3.  Effects of the current used on determining a critical temperature by electrical resistivity measurements in dental alloys.

Authors:  K Hisatsune; Y Tanaka; K Udoh; A M el-Araby; K Iwanuma; K Yasuda
Journal:  Dent Mater J       Date:  1993-12       Impact factor: 2.102

4.  Aging reactions in a low gold, white dental alloy.

Authors:  K Hisatsune; M Ohta; T Shiraishi; M Yamane
Journal:  J Dent Res       Date:  1982-06       Impact factor: 6.116

5.  Age-hardening mechanisms in a commercial dental gold alloy containing platinum and palladium.

Authors:  T Tani; K Udoh; K Yasuda; G Van Tendeloo; J Van Landuyt
Journal:  J Dent Res       Date:  1991-10       Impact factor: 6.116

6.  Hardening of gold-based alloys.

Authors:  K F Leinfelder; D F Taylor
Journal:  J Dent Res       Date:  1977-03       Impact factor: 6.116