Literature DB >> 17483886

FT-IR spectroscopy of fluoro-substituted hydroxyapatite: strengths and limitations.

Llew Rintoul1, Edeline Wentrup-Byrne, Shuko Suzuki, Lisbeth Grøndahl.   

Abstract

Fluoro substituted hydroxyapatite (FHAp) samples were prepared by a cyclic pH method. Both calcined and uncalcined samples were subjected to elemental analysis (F, Ca, P) and X-ray diffraction (XRD) analysis to verify composition and phase purity. Good correlation between a-axis parameters and fluoride ion content was found for calcined samples, however, for uncalcined samples the fluoride ion content was higher than estimated from the a-axis values. Fourier transform infra red (FT-IR) spectroscopy analysis of the calcined samples showed OH band shifts and splitting in accordance with F-HO interactions affecting the OH vibration. We conclude that the OH libration (620-780 cm(-1) range) is more suited for estimation of fluoride ion content than the OH stretching. In contrast, uncalcined samples all displayed FT-IR spectra similar to that of hydroxyapatite (HAp) despite the presence of fluoride ions (18-73%). FT-IR emission spectroscopy was used to probe the changes occurring in the FT-IR spectra of HAp and FHAp samples upon heating. Interpretation of the spectral changes occurring during heating to 1,000 degrees C and subsequent cooling is given. Room temperature spectra of samples heated to various temperatures was used to determine the temperature necessary to produce FT-IR spectra displaying the expected OH bands. A model accounting for the combined observations is proposed.

Entities:  

Mesh:

Substances:

Year:  2007        PMID: 17483886     DOI: 10.1007/s10856-007-3052-3

Source DB:  PubMed          Journal:  J Mater Sci Mater Med        ISSN: 0957-4530            Impact factor:   3.896


  8 in total

1.  An infrared and x-ray diffractometric study of the incorporation of fluoride into hydorxyapatite under conditions of the cyclic variation of pH.

Authors:  E J Duff
Journal:  Arch Oral Biol       Date:  1975-11       Impact factor: 2.633

2.  Preparation and characterization of fluoride-substituted apatites.

Authors:  L J Jha; S M Best; J C Knowles; I Rehman; J D Santos; W Bonfield
Journal:  J Mater Sci Mater Med       Date:  1997-04       Impact factor: 3.896

3.  Fourier transform infrared spectrometry: a versatile technique for real world samples.

Authors:  L Rintoul; H Panayiotou; S Kokot; G George; G Cash; R Frost; T Bui; P Fredericks
Journal:  Analyst       Date:  1998-04       Impact factor: 4.616

4.  Degradation of hydroxylapatite, fluorapatite, and fluorhydroxyapatite coatings of dental implants in dogs.

Authors:  L Gineste; M Gineste; X Ranz; A Ellefterion; A Guilhem; N Rouquet; P Frayssinet
Journal:  J Biomed Mater Res       Date:  1999

5.  Mechanism for fluorine inhibition of diffusion in hydroxyapatite.

Authors:  R A Young; W van der Lugt; J C Elliott
Journal:  Nature       Date:  1969-08-16       Impact factor: 49.962

6.  Synthesis and characterization of fluorine-containing hydroxyapatite by a pH-cycling method.

Authors:  H Qu; M Wei
Journal:  J Mater Sci Mater Med       Date:  2005-02       Impact factor: 3.896

7.  Synthesis and characterization of hydroxyapatite, fluoride-substituted hydroxyapatite and fluorapatite.

Authors:  M Wei; J H Evans; T Bostrom; L Grøndahl
Journal:  J Mater Sci Mater Med       Date:  2003-04       Impact factor: 3.896

8.  Variability of hydroxyapatite preparations.

Authors:  R A Young; D W Holcomb
Journal:  Calcif Tissue Int       Date:  1982       Impact factor: 4.333

  8 in total
  6 in total

1.  Alteration of dentin-enamel mechanical properties due to dental whitening treatments.

Authors:  B Zimmerman; L Datko; M Cupelli; S Alapati; D Dean; M Kennedy
Journal:  J Mech Behav Biomed Mater       Date:  2010-02-21

2.  Effects of fluoridation of porcine hydroxyapatite on osteoblastic activity of human MG63 cells.

Authors:  Zhipeng Li; Baoxin Huang; Sui Mai; Xiayi Wu; Hanqing Zhang; Wei Qiao; Xin Luo; Zhuofan Chen
Journal:  Sci Technol Adv Mater       Date:  2015-06-02       Impact factor: 8.090

3.  In vivo study and thermodynamic investigation of two lanthanum complexes, La(dpp)3 and La(XT), for the treatment of bone resorption disorders.

Authors:  J F Cawthray; D M Weekes; O Sivak; A L Creagh; F Ibrahim; M Iafrate; C A Haynes; K M Wasan; C Orvig
Journal:  Chem Sci       Date:  2015-08-03       Impact factor: 9.825

4.  Effect of mechanochemical activation of natural phosphorite structure as well as phosphorus solubility.

Authors:  Nana Fang; Yuanliang Shi; Zhenhua Chen; Xun Sun; Lei Zhang; Yanli Yi
Journal:  PLoS One       Date:  2019-11-07       Impact factor: 3.240

5.  In-vitro bioactivity evaluation and physical properties of an epoxy-based dental sealer reinforced with synthesized fluorine-substituted hydroxyapatite, hydroxyapatite and bioactive glass nanofillers.

Authors:  Bahaa Abdulrazzaq Jerri Al-Bakhsh; Farhad Shafiei; Atieh Hashemian; Kiana Shekofteh; Behnam Bolhari; Marjan Behroozibakhsh
Journal:  Bioact Mater       Date:  2019-10-28

6.  Excess heat capacity and entropy of mixing along the hydroxyapatite-chlorapatite and hydroxyapatite-fluorapatite binaries.

Authors:  Edgar Dachs; Artur Benisek; Daniel Harlov; Max Wilke
Journal:  Phys Chem Miner       Date:  2021-10-28       Impact factor: 1.342

  6 in total

北京卡尤迪生物科技股份有限公司 © 2022-2023.