Silk fibroin (SF)/poly(vinyl alcohol) (PVA) blend filaments were prepared by a wet spinning process. Regenerated SF and PVA were dissolved in formic acid and the dope solution exhibited good fiber formation in a methanol coagulation bath. Due to the miscibility of SF/PVA in formic acid, the filament had a smooth surface and dense structure with a circular cross-section. The crystalline structure and thermal properties were varied with different SF/PVA ratios. The mechanical properties of the filament were also controlled by blending PVA with SF. Especially, the knot strength of the SF filament, which is a very important suture property, could be significantly improved by blending with PVA.Entities: